General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4.9 % Show Supplier Material materials with Absorción de agua of 4.9 % | dry | Sim. to ISO 62 |
Densidad | 1.43 g/cm³ Show Supplier Material materials with Densidad of 1.43 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | dry | ISO 527-1/-2 |
4.5 % Show Supplier Material materials with Elongación of 4.5 % | dry | ISO 527-1/-2 | ||
8.3 % Show Supplier Material materials with Elongación of 8.3 % | conditioned | ISO 527-1/-2 | ||
120 °C | 11.7 % Show Supplier Material materials with Elongación of 11.7 % | dry | ISO 527-1/-2 | |
150 °C | 12.2 % Show Supplier Material materials with Elongación of 12.2 % | dry | ISO 527-1/-2 | |
160 °C | 12.3 % Show Supplier Material materials with Elongación of 12.3 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | conditioned | ISO 178 | |
295 MPa Show Supplier Material materials with Flexural yield strength of 295 MPa | dry | ISO 178 | ||
Módulo de flexión | 7 GPa Show Supplier Material materials with Módulo de flexión of 7 GPa | conditioned | ISO 178 | |
11.2 GPa Show Supplier Material materials with Módulo de flexión of 11.2 GPa | dry | ISO 178 | ||
Módulo elástico | -40 °C | 12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | ISO 527-1/-2 |
6.5 GPa Show Supplier Material materials with Módulo elástico of 6.5 GPa | conditioned | ISO 527-1/-2 | ||
11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | ||
40 °C | 10.5 GPa Show Supplier Material materials with Módulo elástico of 10.5 GPa | dry | ISO 527-1/-2 | |
100 °C | 5.1 GPa Show Supplier Material materials with Módulo elástico of 5.1 GPa | dry | ISO 527-1/-2 | |
120 °C | 4.8 GPa Show Supplier Material materials with Módulo elástico of 4.8 GPa | dry | ISO 527-1/-2 | |
150 °C | 4.2 GPa Show Supplier Material materials with Módulo elástico of 4.2 GPa | dry | ISO 527-1/-2 | |
160 °C | 4.1 GPa Show Supplier Material materials with Módulo elástico of 4.1 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 275 MPa Show Supplier Material materials with Resistencia a la tracción of 275 MPa | dry | ISO 527-1/-2 |
125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | conditioned | ISO 527-1/-2 | ||
175 MPa Show Supplier Material materials with Resistencia a la tracción of 175 MPa | dry | ISO 527-1/-2 | ||
100 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | dry | ISO 527-1/-2 | |
120 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | |
150 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | dry | ISO 527-1/-2 | |
160 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | dry | ISO 179/1eA | |
23 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 35 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 110 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 110 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 105 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 105 kJ/m² | dry | ISO 179/1eU | |
23 °C | 110 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 110 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 1.15e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.15e-07 mm²/s | dry | - | ||
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | dry | ISO 75-1/-2 | 2 MPa | |
215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.3 [-] Show Supplier Material materials with Constante dieléctrica of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Constante dieléctrica of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Constante dieléctrica of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Constante dieléctrica of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 90 [-] Show Supplier Material materials with Factor de disipación of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Factor de disipación of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Factor de disipación of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | conditioned | IEC 60243-1 | |
25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | conditioned | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.35 % Show Supplier Material materials with Contracción of 0.35 % | dry | ISO 294-4 | Parallel | |
0.81 % Show Supplier Material materials with Contracción of 0.81 % | dry | ISO 294-4 | Normal | ||
Density of melt | 1280 g/cm³ Show Supplier Material materials with Density of melt of 1280 g/cm³ | dry | - | ||
Specific heat capacity melt | 2010.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2010.0 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.3 W/(m·K) | dry | - | ||
Velocidad de flujo de la masa derretida | 21 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 21 g/10min | dry | ISO 1133 | ||
Velocidad de flujo del volumen derretido | 275 °C | 14.0 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 14.0 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Chair Bases, Chair Arms, Chair Frames, Oil Sumps and Pans, Airbag Containers, Suspension System Spring Seats, Refrigerator hinge | |
Fillers | 40% Glass Fiber |