General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.69 g/cm³ Show Supplier Material materials with Densidad of 1.69 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 1.5 % Show Supplier Material materials with Elongación of 1.5 % | dry | ISO 527-1/-2 |
2.2 % Show Supplier Material materials with Elongación of 2.2 % | dry | ISO 527-1/-2 | ||
3.3 % Show Supplier Material materials with Elongación of 3.3 % | conditioned | ISO 527-1/-2 | ||
160 °C | 3.4 % Show Supplier Material materials with Elongación of 3.4 % | dry | ISO 527-1/-2 | |
200 °C | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 255 MPa Show Supplier Material materials with Flexural yield strength of 255 MPa | conditioned | ISO 178 | |
270 MPa Show Supplier Material materials with Flexural yield strength of 270 MPa | dry | ISO 178 | ||
Módulo de flexión | 12 GPa Show Supplier Material materials with Módulo de flexión of 12 GPa | conditioned | ISO 178 | |
12.5 GPa Show Supplier Material materials with Módulo de flexión of 12.5 GPa | dry | ISO 178 | ||
Módulo elástico | -40 °C | 18 GPa Show Supplier Material materials with Módulo elástico of 18 GPa | dry | ISO 527-1/-2 |
10.7 GPa Show Supplier Material materials with Módulo elástico of 10.7 GPa | conditioned | ISO 527-1/-2 | ||
16 GPa Show Supplier Material materials with Módulo elástico of 16 GPa | dry | ISO 527-1/-2 | ||
100 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-1/-2 | |
160 °C | 8.3 GPa Show Supplier Material materials with Módulo elástico of 8.3 GPa | dry | ISO 527-1/-2 | |
200 °C | 7.6 GPa Show Supplier Material materials with Módulo elástico of 7.6 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 220 MPa Show Supplier Material materials with Resistencia a la tracción of 220 MPa | dry | ISO 527-1/-2 |
170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | conditioned | ISO 527-1/-2 | ||
235 MPa Show Supplier Material materials with Resistencia a la tracción of 235 MPa | dry | ISO 527-1/-2 | ||
160 °C | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-1/-2 | |
200 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8.5 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 18 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 18 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | dry | ISO 179/1eU |
-30 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU | |
23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 285 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 285 °C | dry | ISO 75-1/-2 | 2 MPa | |
288 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 288 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 290 °C Show Supplier Material materials with Temperatura de fusión of 290 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de reblandecimiento Vicat | 285 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 285 °C | dry | ISO 306 | 50°C/h 50N | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | dry | Sim. to ISO 294-4 | Parallel |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | Sim. to ISO 294-4 | Normal | |
Spiral flow length | 160 | dry | - | 1.0 mm 800 bar |
170 | dry | - | 1.0 mm 900 bar | |
180 | dry | - | 1.0 mm 1000 bar | |
Viscosity number | 75 cm³/gr Show Supplier Material materials with Viscosity number of 75 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Self propelled lawnmower transmission gears, Transmission Control Gears, Oil Pump Gears (2-wheelers), Crankshaft Balance Gears, Oil Pump Gears (automotive), EPS gears, EPS Steering components: Gears, Flex couplers and Sensors, Gears, Electronic throttle control actuators, Exhaust gas recirculation actuators, Turbo actuators, Coolant valve actuators | |
Fillers | 50% Glass Fiber and PTFE |