General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 3.4 % Show Supplier Material materials with Absorción de agua of 3.4 % | dry | Sim. to ISO 62 |
Densidad | 1.55 g/cm³ Show Supplier Material materials with Densidad of 1.55 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 1.9 % Show Supplier Material materials with Elongación of 1.9 % | dry, conditioned | ISO 527-1/-2 | |
Flexural yield strength | 260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | conditioned | ISO 178 | |
280 MPa Show Supplier Material materials with Flexural yield strength of 280 MPa | dry | ISO 178 | ||
Módulo de flexión | 14.5 GPa Show Supplier Material materials with Módulo de flexión of 14.5 GPa | dry, conditioned | ISO 178 | |
Módulo elástico | 13.5 GPa Show Supplier Material materials with Módulo elástico of 13.5 GPa | dry, conditioned | ISO 527-1/-2 | |
Resistencia a la tracción | 170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry, conditioned | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry, conditioned | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry, conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 300 °C Show Supplier Material materials with Ball pressure temperature of 300 °C | dry | IEC 60695-10-2 | |||
Coeficiente de dilatación térmica | 3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-07 1/K | dry | ASTM D696 | Parallel | ||
3.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.5e-07 1/K | dry | ASTM D696 | Normal | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | ||
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 3 mm | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.35 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.35 mm | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | UL746B | 0.35 mm | ||
Temperatura de flexión bajo carga | 305 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 305 °C | dry | ISO 75-1/-2 | 2 MPa | ||
323 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 323 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 125 °C Show Supplier Material materials with Temperatura de transición del vidrio of 125 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.9 [-] Show Supplier Material materials with Constante dieléctrica of 3.9 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz |
4.2 [-] Show Supplier Material materials with Constante dieléctrica of 4.2 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 50 [-] Show Supplier Material materials with Factor de disipación of 50 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 33 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 33 kV/mm | dry, conditioned | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | ISO 294-4 | Parallel |
0.85 % Show Supplier Material materials with Contracción of 0.85 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 105 | dry | - | 1.0 mm 1000 bar |
Viscosity number | 86 cm³/gr Show Supplier Material materials with Viscosity number of 86 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | MCCB Housings, Industrial Control Gear, Medium Voltage Circuit Breakers, Medium Voltage Circuit Breakers Embedded Pole | |
Certifications | Yellow Card Available | |
Fillers | 40% Glass Fiber |