General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2.3 % Show Supplier Material materials with Absorción de agua of 2.3 % | dry | ISO 62 | at 23°C after 24h |
8.1 % Show Supplier Material materials with Absorción de agua of 8.1 % | dry | Sim. to ISO 62 | ||
Densidad | 1.51 g/cm³ Show Supplier Material materials with Densidad of 1.51 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.2 % Show Supplier Material materials with Moisture absorption of 2.2 % | dry | Sim. to ISO 62 | |
Índice límite de óxigeno | 22 % Show Supplier Material materials with Índice límite de óxigeno of 22 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.3 % Show Supplier Material materials with Elongación of 3.3 % | dry | ISO 527-1/-2 | |
6 % Show Supplier Material materials with Elongación of 6 % | conditioned | ISO 527-1/-2 | ||
120 °C | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | |
160 °C | 7 % Show Supplier Material materials with Elongación of 7 % | dry | ISO 527-1/-2 | |
180 °C | 7 % Show Supplier Material materials with Elongación of 7 % | dry | ISO 527-1/-2 | |
200 °C | 8 % Show Supplier Material materials with Elongación of 8 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 220 MPa Show Supplier Material materials with Flexural yield strength of 220 MPa | conditioned | ISO 178 | |
325 MPa Show Supplier Material materials with Flexural yield strength of 325 MPa | dry | ISO 178 | ||
120 °C | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |
160 °C | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | dry | ISO 178 | |
Módulo de flexión | 7 GPa Show Supplier Material materials with Módulo de flexión of 7 GPa | conditioned | ISO 178 | |
11.8 GPa Show Supplier Material materials with Módulo de flexión of 11.8 GPa | dry | ISO 178 | ||
120 °C | 5.8 GPa Show Supplier Material materials with Módulo de flexión of 5.8 GPa | dry | ISO 178 | |
160 °C | 5.2 GPa Show Supplier Material materials with Módulo de flexión of 5.2 GPa | dry | ISO 178 | |
Módulo elástico | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | conditioned | ISO 527-1/-2 | |
13 GPa Show Supplier Material materials with Módulo elástico of 13 GPa | dry | ISO 527-1/-2 | ||
120 °C | 6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | dry | ISO 527-1/-2 | |
160 °C | 6.1 GPa Show Supplier Material materials with Módulo elástico of 6.1 GPa | dry | ISO 527-1/-2 | |
180 °C | 5.6 GPa Show Supplier Material materials with Módulo elástico of 5.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 5.2 GPa Show Supplier Material materials with Módulo elástico of 5.2 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | conditioned | ISO 527-1/-2 | |
235 MPa Show Supplier Material materials with Resistencia a la tracción of 235 MPa | dry | ISO 527-1/-2 | ||
120 °C | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | ISO 527-1/-2 | |
160 °C | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | dry | ISO 527-1/-2 | |
180 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | dry | ISO 527-1/-2 | |
200 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | dry | ISO 179/1eA | |
23 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 21 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | dry | ISO 179/1eU |
-30 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 95 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 95 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 1.35e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.35e-07 mm²/s | dry | - | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | |
290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de reblandecimiento Vicat | 290 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 290 °C | dry | ISO 306 | 50°C/h 50N | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.4 [-] Show Supplier Material materials with Constante dieléctrica of 4.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.6 [-] Show Supplier Material materials with Constante dieléctrica of 4.6 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
12 [-] Show Supplier Material materials with Constante dieléctrica of 12 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 80 [-] Show Supplier Material materials with Factor de disipación of 80 [-] | dry | IEC 62631-2-1 | 100Hz |
230 [-] Show Supplier Material materials with Factor de disipación of 230 [-] | dry | IEC 62631-2-1 | 1MHz | |
900 [-] Show Supplier Material materials with Factor de disipación of 900 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1500 [-] Show Supplier Material materials with Factor de disipación of 1500 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 400 V Show Supplier Material materials with Índice de seguimiento comparativo of 400 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1320 g/cm³ Show Supplier Material materials with Density of melt of 1320 g/cm³ | dry | - | |
Specific heat capacity melt | 1930 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1930 J/(kg·K) | dry | - | |
Spiral flow length | 80 | dry | - | 1.0 mm 800 bar |
90 | dry | - | 1.0 mm 900 bar | |
100 | dry | - | 1.0 mm 1000 bar | |
Thermal conductivity of melt | 0.344 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.344 W/(m·K) | dry | - | |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 40% Glass Fiber |