Description

Material EN AW-Al 99,8(A) is produced in large quantities for sheets, strips, plates, scraps, rolled bars and wire and prewire for mechanical resp. welding application. It is used in limited quantities for pressed bars as well as for presswork components. It is food-safe. The material is comparable to trademark Al99,8, material number 3.0285, acc. to DIN 1712-3 : 1976-12. EN AW-Al 99,8(A) is well anodizable and shows favorable electrical and thermal conductivity. Smearing may occur on machining. Low mechanical strength, high strain. Formability as well as chemical and weathering resistance are excellent. Application: apparatus engineering, roll bond, Z-bond, household appliances, storage and transport equipment for chemical, pharmaceutical and food industry. Furthermore for roofings, facings, arts-and-crafts, packagings, extruded parts, e.g. collapsible tubes, tubes, cans, bottles.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey,Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

23.0 °C

2.69 - 2.7 g/cm³

Show Material materials with Density of 2.69 - 2.7 g/cm³

Dimension

PropertyValue

Thickness

0.2 - 3 mm

Show Material materials with Thickness of 0.2 - 3 mm

Mechanical

PropertyTemperatureValueComment

Bending angle 180°

23.0 °C

0.5 - 1 °/t

Show Material materials with Bending angle 180° of 0.5 - 1 °/t

according to EN 485-2

Bending angle 90°

23.0 °C

0 - 2 °/t

Show Material materials with Bending angle 90° of 0 - 2 °/t

according to EN 485-2

Elastic modulus

-270.0 °C

70 GPa

Show Material materials with Elastic modulus of 70 GPa

20.0 °C

60 - 70 GPa

Show Material materials with Elastic modulus of 60 - 70 GPa

23.0 °C

70 GPa

Show Material materials with Elastic modulus of 70 GPa

50.0 °C

69 GPa

Show Material materials with Elastic modulus of 69 GPa

100.0 °C

68 GPa

Show Material materials with Elastic modulus of 68 GPa

150.0 °C

66 GPa

Show Material materials with Elastic modulus of 66 GPa

200.0 °C

63 GPa

Show Material materials with Elastic modulus of 63 GPa

250.0 °C

57 GPa

Show Material materials with Elastic modulus of 57 GPa

300.0 °C

50 GPa

Show Material materials with Elastic modulus of 50 GPa

Unlock all property charts

Elongation A50

20.0 °C

5 - 12 %

Show Material materials with Elongation A50 of 5 - 12 %

according to EN 485-2

23.0 °C

2 - 12 %

Show Material materials with Elongation A50 of 2 - 12 %

according to EN 485-2

Unlock all property charts

Elongation A50, transverse

20.0 °C

5 - 12 %

Show Material materials with Elongation A50, transverse of 5 - 12 %

Hardness, Brinell

20.0 °C

26 [-]

Show Material materials with Hardness, Brinell of 26 [-]

23.0 °C

26 [-]

Show Material materials with Hardness, Brinell of 26 [-]

Unlock all property charts

Hardness, HBW

23.0 °C

26 - 36 [-]

Show Material materials with Hardness, HBW of 26 - 36 [-]

according to EN 485-2

Plane-Strain Fracture Toughnes

23.0 °C

22 - 35 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 1000 Series Aluminium

Shear modulus

20.0 °C

25 GPa

Show Material materials with Shear modulus of 25 GPa

23.0 °C

26.5 GPa

Show Material materials with Shear modulus of 26.5 GPa

Unlock all property charts

Tensile strength

20.0 °C

80 - 120 MPa

Show Material materials with Tensile strength of 80 - 120 MPa

according to EN 485-2

23.0 °C

80 - 150 MPa

Show Material materials with Tensile strength of 80 - 150 MPa

according to EN 485-2

Unlock all property charts

Tensile strength, transverse

20.0 °C

80 - 120 MPa

Show Material materials with Tensile strength, transverse of 80 - 120 MPa

Yield strength

23.0 °C

55 - 90 MPa

Show Material materials with Yield strength of 55 - 90 MPa

according to EN 485-2

Yield strength Rp0.2

20.0 °C

55 MPa

Show Material materials with Yield strength Rp0.2 of 55 MPa

23.0 °C

55 MPa

Show Material materials with Yield strength Rp0.2 of 55 MPa

Unlock all property charts

Yield strength Rp0.2, transverse

20.0 °C

55 MPa

Show Material materials with Yield strength Rp0.2, transverse of 55 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

2.35E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.35E-5 1/K

20-100°C

100.0 °C

2.3E-5 - 2.35E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.3E-5 - 2.35E-5 1/K

20-100°C

Unlock all property charts

Melting point

659 °C

Show Material materials with Melting point of 659 °C

Specific heat capacity

20.0 °C

921 J/(kg·K)

Show Material materials with Specific heat capacity of 921 J/(kg·K)

Thermal conductivity

20.0 °C

215 W/(m·K)

Show Material materials with Thermal conductivity of 215 W/(m·K)

23.0 °C

138 - 225 W/(m·K)

Show Material materials with Thermal conductivity of 138 - 225 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

3.64E+7 - 3.70E+7 S/m

Show Material materials with Electrical conductivity of 3.64E+7 - 3.70E+7 S/m

23.0 °C

3.45E+7 - 3.50E+7 S/m

Show Material materials with Electrical conductivity of 3.45E+7 - 3.50E+7 S/m

Unlock all property charts

Electrical resistivity

23.0 °C

2.86E-8 - 4.9E-8 Ω·m

Show Material materials with Electrical resistivity of 2.86E-8 - 4.9E-8 Ω·m

Chemical properties

PropertyValueComment

Aluminium

99.8 %

Show Material materials with Aluminium of 99.8 %

Copper

0.03 %

Show Material materials with Copper of 0.03 %

Gallium

0.03 %

Show Material materials with Gallium of 0.03 %

Iron

0.15 %

Show Material materials with Iron of 0.15 %

Magnesium

0.02 %

Show Material materials with Magnesium of 0.02 %

Manganese

0.02 %

Show Material materials with Manganese of 0.02 %

Other

0.02 %

Show Material materials with Other of 0.02 %

each 0.02,Min.

Silicon

0.15 %

Show Material materials with Silicon of 0.15 %

Titanium

0.02 %

Show Material materials with Titanium of 0.02 %

Zinc

0.06 %

Show Material materials with Zinc of 0.06 %

Technological properties

Property
Anodizing

decorative: very good, Protective: very good

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetic pieces; Automotive trim: Interior trim, Windows frame, Marque badges

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Corrosion properties

Excellent

Welding

Excellent

Workability

Bending / Spinning (cold): very good / very good, Impact extrusion (cold): very good, Deep drawing / upsetting (Condition) very good (H14) / very good (H12)