General
Property | Value | Temperature |
---|---|---|
Density | 2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Bending Fatigue Strength | 90 MPa Show Material materials with Bending Fatigue Strength of 90 MPa at 23.0 °C | 23.0 °C | |
Elastic modulus | 69 GPa Show Material materials with Elastic modulus of 69 GPa at 23.0 °C | 23.0 °C | |
Elongation A50 | 4 - 9 % Show Material materials with Elongation A50 of 4 - 9 % at 23.0 °C | 23.0 °C | |
Hardness, Brinell | 46 [-] Show Material materials with Hardness, Brinell of 46 [-] at 23.0 °C | 23.0 °C | |
Plane-Strain Fracture Toughnes | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Shear modulus | 26 - 26.5 GPa Show Material materials with Shear modulus of 26 - 26.5 GPa at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Tensile strength | 150 - 195 MPa Show Material materials with Tensile strength of 150 - 195 MPa at 23.0 °C | 23.0 °C | |
Yield strength Rp0.2 | 110 - 145 MPa Show Material materials with Yield strength Rp0.2 of 110 - 145 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 2.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.38E-5 1/K at 20.0 °C | 20.0 °C | |
2.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.38E-5 1/K at 100.0 °C | 100.0 °C | ||
Max service temperature | 150 °C Show Material materials with Max service temperature of 150 °C | Typical for Wrought 5000 Series Aluminium | |
Melting point | 625 - 650 °C Show Material materials with Melting point of 625 - 650 °C | ||
Specific heat capacity | 879 - 963 J/(kg·K) Show Material materials with Specific heat capacity of 879 - 963 J/(kg·K) at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Thermal conductivity | 193 W/(m·K) Show Material materials with Thermal conductivity of 193 W/(m·K) at 23.0 °C | 23.0 °C |
Electrical
Property | Value | Temperature |
---|---|---|
Electrical conductivity | 2.90E+7 S/m Show Material materials with Electrical conductivity of 2.90E+7 S/m at 23.0 °C | 23.0 °C |
Electrical resistivity | 3.45E-8 Ω·m Show Material materials with Electrical resistivity of 3.45E-8 Ω·m at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Chromium | 0.1 % | |
Copper | 0.2 % | |
Iron | 0.7 % | |
Magnesium | 1.1 - 1.8 % | |
Manganese | 0.1 % | |
Other | each 0.05, total 0.15, Rest Al | |
Silicon | 0.4 % | |
Zinc | 0.25 % |
Technological properties
Property | ||
---|---|---|
Brazing | general: Lötbar mit speziellen Techniken oder bei bestimmten Anwendungen | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: not suitable (O), poor (H32, H34), sufficient (H36, H38) | |
Workability | general (condition): good (O, H32), acceptable (H34), poor(H36, H38) |