General
Property | Value | Temperature |
---|---|---|
Density | 2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ at 20.0 °C | 20.0 °C |
2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ at 23.0 °C | 23.0 °C | |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 70 GPa Show Material materials with Elastic modulus of 70 GPa at 23.0 °C | 23.0 °C | |
Elongation | 3 % Show Material materials with Elongation of 3 % at 23.0 °C | 23.0 °C | |
Elongation A100 | 3 % Show Material materials with Elongation A100 of 3 % at 20.0 °C | 20.0 °C | |
Plane-Strain Fracture Toughnes | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Shear modulus | 26.5 GPa Show Material materials with Shear modulus of 26.5 GPa at 20.0 °C | 20.0 °C | |
Tensile strength | 245 MPa Show Material materials with Tensile strength of 245 MPa at 20.0 °C | 20.0 °C | |
245 MPa Show Material materials with Tensile strength of 245 MPa at 23.0 °C | 23.0 °C | ||
Yield strength Rp0.2 | 200 MPa Show Material materials with Yield strength Rp0.2 of 200 MPa at 20.0 °C | 20.0 °C | |
200 MPa Show Material materials with Yield strength Rp0.2 of 200 MPa at 23.0 °C | 23.0 °C | ||
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 2.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.38E-5 1/K at 20.0 °C | 20.0 °C | |
2.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.38E-5 1/K at 100.0 °C | 100.0 °C | ||
Max service temperature | 150 °C Show Material materials with Max service temperature of 150 °C | Typical for Wrought 5000 Series Aluminium | |
Melting point | 560 - 655 °C Show Material materials with Melting point of 560 - 655 °C | Typical for Wrought 5000 Series Aluminium | |
Specific heat capacity | 921 J/(kg·K) Show Material materials with Specific heat capacity of 921 J/(kg·K) at 20.0 °C | 20.0 °C | |
Thermal conductivity | 135 - 167 W/(m·K) Show Material materials with Thermal conductivity of 135 - 167 W/(m·K) at 20.0 °C | 20.0 °C |
Electrical
Property | Value | Temperature | Comment |
---|---|---|---|
Electrical conductivity | 2.20E+7 - 2.60E+7 S/m Show Material materials with Electrical conductivity of 2.20E+7 - 2.60E+7 S/m at 20.0 °C | 20.0 °C | |
Electrical resistivity | 3.3E-8 - 5E-8 Ω·m Show Material materials with Electrical resistivity of 3.3E-8 - 5E-8 Ω·m at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | ||
---|---|---|
Chromium | 0.3 % | |
Copper | 0.05 % | |
Iron | 0.45 % | |
Magnesium | 1.4 - 2.1 % | |
Manganese | 0.25 % | |
Other | each 0.05, total 0.15, Rest Al | |
Silicon | 0.3 % | |
Titanium | 0.1 % | |
Zinc | 0.2 % |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): ausreichend - ungeeignet / mangelhaft, friction soldering: good, soft brazing with flux: sufficient | |
Corrosion properties | Seawater: good, weathering: very good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) good (O) / acceptable (H12) |