Description

Aluminum EN AW-5052 is a non-heat treatable alloy with excellent finishing qualities. EN AW-5052 offers better corrosion resistance than most aluminum alloys, especially to salt water and marine atmospheres. This alloy can be readily welded using most common techniques and is in fact offers some of the best welding characteristics of all aluminum alloys.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

2.68 - 2.69 g/cm³

Show Material materials with Density of 2.68 - 2.69 g/cm³

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

2.69 g/cm³

Show Material materials with Density of 2.69 g/cm³

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Elongation

13.0 %

Show Material materials with Elongation of 13.0 %

F

EN 573-3, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

A50

15.0 %

Show Material materials with Elongation of 15.0 %

F

EN 573-3, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

A100

20.0 °C

13.0 %

Show Material materials with Elongation of 13.0 %

F

EN 573-3

Profile, Rod, Tube

A50

20.0 °C

15.0 %

Show Material materials with Elongation of 15.0 %

F

EN 573-3

Profile, Rod, Tube

Unlock all property charts

Hardness, Brinell

20.0 °C

47.0 [-]

Show Material materials with Hardness, Brinell of 47.0 [-]

F

EN 573-3

Profile, Rod, Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

20.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Shear modulus

26.3 GPa

Show Material materials with Shear modulus of 26.3 GPa

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

26.3 - 27.0 GPa

Show Material materials with Shear modulus of 26.3 - 27.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

26.3 GPa

Show Material materials with Shear modulus of 26.3 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Tensile strength

165.0 MPa

Show Material materials with Tensile strength of 165.0 MPa

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

170.0 MPa

Show Material materials with Tensile strength of 170.0 MPa

F

EN 573-3, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

180.0 - 250.0 MPa

Show Material materials with Tensile strength of 180.0 - 250.0 MPa

F

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

165.0 MPa

Show Material materials with Tensile strength of 165.0 MPa

F

EN 573-3

Flat

20.0 °C

165.0 MPa

Show Material materials with Tensile strength of 165.0 MPa

F

EN 573-3

Flat

Transverse

20.0 °C

170.0 MPa

Show Material materials with Tensile strength of 170.0 MPa

F

EN 573-3

Profile, Rod, Tube

Unlock all property charts

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

-50.0 °C

2.21e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.21e-05 1/K

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

-50 °C

2.2100000000000002e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2100000000000002e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20 °C

2.2100000000000002e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2100000000000002e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20 °C

2.48e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.48e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20 °C

2.5699999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5699999999999998e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

100 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

100.0 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

200 °C

2.48e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.48e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

200.0 °C

2.48e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.48e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

300 °C

2.5699999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5699999999999998e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

300.0 °C

2.57e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.57e-05 1/K

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

605.0 - 650.0 °C

Show Material materials with Melting point of 605.0 - 650.0 °C

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

607.0 - 649.0 °C

Show Material materials with Melting point of 607.0 - 649.0 °C

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

900.0 - 901.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 - 901.0 J/(kg·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

901.0 J/(kg·K)

Show Material materials with Specific heat capacity of 901.0 J/(kg·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Thermal conductivity

138 W/(m·K)

Show Material materials with Thermal conductivity of 138 W/(m·K)

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

130.0 - 150.0 W/(m·K)

Show Material materials with Thermal conductivity of 130.0 - 150.0 W/(m·K)

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20.0 °C

130.0 - 138.0 W/(m·K)

Show Material materials with Thermal conductivity of 130.0 - 138.0 W/(m·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

138.0 - 150.0 W/(m·K)

Show Material materials with Thermal conductivity of 138.0 - 150.0 W/(m·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

138.0 W/(m·K)

Show Material materials with Thermal conductivity of 138.0 W/(m·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20000000.0 S/m

Show Material materials with Electrical conductivity of 20000000.0 S/m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

19000000.0 - 21000000.0 S/m

Show Material materials with Electrical conductivity of 19000000.0 - 21000000.0 S/m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

Electrical resistivity

4.76e-08 - 5.26e-08 Ω·m

Show Material materials with Electrical resistivity of 4.76e-08 - 5.26e-08 Ω·m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

5e-08 Ω·m

Show Material materials with Electrical resistivity of 5e-08 Ω·m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

4.7e-08 - 4.95e-08 Ω·m

Show Material materials with Electrical resistivity of 4.7e-08 - 4.95e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

4.7e-08 - 5.2e-08 Ω·m

Show Material materials with Electrical resistivity of 4.7e-08 - 5.2e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

4.95e-08 Ω·m

Show Material materials with Electrical resistivity of 4.95e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

4.95e-08 - 5.2e-08 Ω·m

Show Material materials with Electrical resistivity of 4.95e-08 - 5.2e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.15 - 0.35 %

Show Material materials with Chromium of 0.15 - 0.35 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Plate, Strip, Sheet, Foil, Wire, Bar

Copper

0.1 %

Show Material materials with Copper of 0.1 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Plate, Strip, Sheet, Foil, Wire, Bar

Iron

0.4 %

Show Material materials with Iron of 0.4 %

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

0.40 %

Show Material materials with Iron of 0.40 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Magnesium

2.2 - 2.8 %

Show Material materials with Magnesium of 2.2 - 2.8 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Plate, Strip, Sheet, Foil, Wire, Bar

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Plate, Strip, Sheet, Foil, Wire, Bar

Silicon

0.25 %

Show Material materials with Silicon of 0.25 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Plate, Strip, Sheet, Foil, Wire, Bar

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Plate, Strip, Sheet, Foil, Wire, Bar

Technological properties

Property
Anodizing

decorative: good, Protective: very good

Corrosion properties

Seawater: very good to good, weathering: good

Workability