General
Property | Value | Condition | Related Standards |
---|---|---|---|
Density | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | H12 | AA Standards |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 68.0 - 70.0 GPa Show Material materials with Elastic modulus of 68.0 - 70.0 GPa | Typical for Wrought 1000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 1000 Series Aluminium |
Shear modulus | 25.9 GPa Show Material materials with Shear modulus of 25.9 GPa | Typical for Wrought 1000 Series Aluminium |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 1000 Series Aluminium |
Melting point | 645.0 - 660.0 °C Show Material materials with Melting point of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Specific heat capacity | 900.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium |
Thermal conductivity | 167.0 - 244.0 W/(m·K) Show Material materials with Thermal conductivity of 167.0 - 244.0 W/(m·K) | Typical for Wrought 1000 Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 33000000.0 - 38000000.0 S/m Show Material materials with Electrical conductivity of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
Electrical resistivity | 2.7e-08 - 3e-08 Ω·m Show Material materials with Electrical resistivity of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 99.99 % Show Material materials with Aluminium of 99.99 % | H12 | AA Standards |
Copper | 0.006 % Show Material materials with Copper of 0.006 % | H12 | AA Standards |
Gallium | 0.005 % Show Material materials with Gallium of 0.005 % | H12 | AA Standards |
Iron | 0.006 % Show Material materials with Iron of 0.006 % | H12 | AA Standards |
Magnesium | 0.006 % Show Material materials with Magnesium of 0.006 % | H12 | AA Standards |
Manganese | 0.002 % Show Material materials with Manganese of 0.002 % | H12 | AA Standards |
Silicon | 0.006 % Show Material materials with Silicon of 0.006 % | H12 | AA Standards |
Titanium | 0.002 % Show Material materials with Titanium of 0.002 % | H12 | AA Standards |
Vanadium | 0.005 % Show Material materials with Vanadium of 0.005 % | H12 | AA Standards |
Zinc | 0.006 % Show Material materials with Zinc of 0.006 % | H12 | AA Standards |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |