General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 2.68 - 2.69 g/cm³ Show Material materials with Density of 2.68 - 2.69 g/cm³ |
23.0 °C | 2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Bending Fatigue Strength | 23.0 °C | 120 MPa Show Material materials with Bending Fatigue Strength of 120 MPa | |
Elastic modulus | 20.0 °C | 70 GPa Show Material materials with Elastic modulus of 70 GPa | |
23.0 °C | 70 GPa Show Material materials with Elastic modulus of 70 GPa | ||
Elongation A50 | 20.0 °C | 4 - 6 % Show Material materials with Elongation A50 of 4 - 6 % | |
23.0 °C | 4 - 7 % Show Material materials with Elongation A50 of 4 - 7 % | ||
Elongation A50, transverse | 20.0 °C | 4 - 6 % Show Material materials with Elongation A50, transverse of 4 - 6 % | |
Plane-Strain Fracture Toughnes | 23.0 °C | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m | Typical for Wrought 5000 Series Aluminium |
Poisson's ratio | 20.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | |
Shear modulus | 20.0 °C | 26.3 - 27 GPa Show Material materials with Shear modulus of 26.3 - 27 GPa | |
23.0 °C | 26.3 GPa Show Material materials with Shear modulus of 26.3 GPa | ||
Tensile strength | 20.0 °C | 230 - 280 MPa Show Material materials with Tensile strength of 230 - 280 MPa | |
23.0 °C | 215 - 280 MPa Show Material materials with Tensile strength of 215 - 280 MPa | ||
Tensile strength, transverse | 20.0 °C | 230 - 280 MPa Show Material materials with Tensile strength, transverse of 230 - 280 MPa | |
Yield strength Rp0.2 | 20.0 °C | 150 - 240 MPa Show Material materials with Yield strength Rp0.2 of 150 - 240 MPa | |
23.0 °C | 150 - 240 MPa Show Material materials with Yield strength Rp0.2 of 150 - 240 MPa | ||
Yield strength Rp0.2, transverse | 20.0 °C | 150 MPa Show Material materials with Yield strength Rp0.2, transverse of 150 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | -50.0 °C | 2.21E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.21E-5 1/K | |
20.0 °C | 2.21E-5 - 2.57E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.21E-5 - 2.57E-5 1/K | ||
100.0 °C | 2.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.38E-5 1/K | ||
200.0 °C | 2.48E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.48E-5 1/K | ||
300.0 °C | 2.57E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.57E-5 1/K | ||
Max service temperature | 150 °C Show Material materials with Max service temperature of 150 °C | Typical for Wrought 5000 Series Aluminium | |
Melting point | 605 - 650 °C Show Material materials with Melting point of 605 - 650 °C | ||
Specific heat capacity | 20.0 °C | 900 - 901 J/(kg·K) Show Material materials with Specific heat capacity of 900 - 901 J/(kg·K) | |
23.0 °C | 900 J/(kg·K) Show Material materials with Specific heat capacity of 900 J/(kg·K) | ||
Thermal conductivity | 20.0 °C | 130 - 150 W/(m·K) Show Material materials with Thermal conductivity of 130 - 150 W/(m·K) | |
23.0 °C | 130 - 150 W/(m·K) Show Material materials with Thermal conductivity of 130 - 150 W/(m·K) | ||
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 1.90E+7 - 2.10E+7 S/m Show Material materials with Electrical conductivity of 1.90E+7 - 2.10E+7 S/m |
23.0 °C | 1.90E+7 - 2.10E+7 S/m Show Material materials with Electrical conductivity of 1.90E+7 - 2.10E+7 S/m | |
Electrical resistivity | 20.0 °C | 4.7E-8 - 5.2E-8 Ω·m Show Material materials with Electrical resistivity of 4.7E-8 - 5.2E-8 Ω·m |
23.0 °C | 4.76E-8 - 5.26E-8 Ω·m Show Material materials with Electrical resistivity of 4.76E-8 - 5.26E-8 Ω·m | |
Chemical properties
Property | Value |
---|---|
Chromium | 0.15 - 0.35 % Show Material materials with Chromium of 0.15 - 0.35 % |
Copper | 0.1 % Show Material materials with Copper of 0.1 % |
Iron | 0.4 % Show Material materials with Iron of 0.4 % |
Magnesium | 2.2 - 2.8 % Show Material materials with Magnesium of 2.2 - 2.8 % |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % |
Other | each 0.05, total 0.15, Rest Al |
Silicon | 0.25 % Show Material materials with Silicon of 0.25 % |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: good, Protective: very good | |
Corrosion properties | Seawater: very good to good, weathering: good | |
Workability | Bending / Spinning (cold): very good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) good (O) / good (H12) |