AA Standards Grade 5052 O

Want to keep this datasheet? Save it now in your required format

Description

Aluminum AA 5052 is a non-heat treatable alloy with excellent finishing qualities. AA 5052 offers better corrosion resistance than most aluminum alloys, especially to salt water and marine atmospheres. This alloy can be readily welded using most common techniques and is in fact offers some of the best welding characteristics of all aluminum alloys.

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated Standards

Density

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Mechanical

PropertyValueConditionRelated StandardsComment

Bending Fatigue Strength

110.0 MPa

Show Material materials with Bending Fatigue Strength of 110.0 MPa

O

AA Standards

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Hardness, Brinell

47.0 [-]

Show Material materials with Hardness, Brinell of 47.0 [-]

O

AA Standards

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Tensile strength

195.0 MPa

Show Material materials with Tensile strength of 195.0 MPa

O

AA Standards

170.0 - 215.0 MPa

Show Material materials with Tensile strength of 170.0 - 215.0 MPa

O

AA Standards, ASTM B209, ASTM B313, ASTM B547

170.0 - 240.0 MPa

Show Material materials with Tensile strength of 170.0 - 240.0 MPa

O

AA Standards, ASTM B210, ASTM B221, ASTM B241

170.0 - 220.0 MPa

Show Material materials with Tensile strength of 170.0 - 220.0 MPa

O

AA Standards, ASTM B211

220.0 MPa

Show Material materials with Tensile strength of 220.0 MPa

O

AA Standards, ASTM B316

170.0 MPa

Show Material materials with Tensile strength of 170.0 MPa

O

AA Standards, ASTM B483

Thermal

PropertyTemperatureValueConditionRelated StandardsComment

Coefficient of thermal expansion

100 °C, 20 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

605.0 - 650.0 °C

Show Material materials with Melting point of 605.0 - 650.0 °C

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Specific heat capacity

879.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K)

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

138 W/(m·K)

Show Material materials with Thermal conductivity of 138 W/(m·K)

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Electrical

PropertyValueConditionRelated Standards

Electrical conductivity

20000000.0 S/m

Show Material materials with Electrical conductivity of 20000000.0 S/m

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Electrical resistivity

5e-08 Ω·m

Show Material materials with Electrical resistivity of 5e-08 Ω·m

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Chemical properties

PropertyValueConditionRelated Standards

Chromium

0.15 - 0.35 %

Show Material materials with Chromium of 0.15 - 0.35 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Copper

0.1 %

Show Material materials with Copper of 0.1 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Iron

0.40 %

Show Material materials with Iron of 0.40 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Magnesium

2.2 - 2.8 %

Show Material materials with Magnesium of 2.2 - 2.8 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Silicon

0.25 %

Show Material materials with Silicon of 0.25 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B483, ASTM B547

Technological properties

Property
Brazing

general: limited brazing

Corrosion properties

Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere

General machinability

General: poor (O, H32), sufficient (H34, H36, H38)

Workability

general (condition): good (O), acceptable (H32, H34), poor(H36, H38)