EN 573-3 Grade AW-5110 F

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.69 g/cm³

Show Material materials with Density of 2.69 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

69 - 70 GPa

Show Material materials with Elastic modulus of 69 - 70 GPa

Typical for Wrought 5000 Series Aluminium

Hardness, Brinell

23.0 °C

27 [-]

Show Material materials with Hardness, Brinell of 27 [-]

Plane-Strain Fracture Toughnes

23.0 °C

22 - 35 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

23.0 °C

26 - 26.5 GPa

Show Material materials with Shear modulus of 26 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.2E-5 - 2.5E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.5E-5 1/K

Typical for Wrought 5000 Series Aluminium

Max service temperature

150 °C

Show Material materials with Max service temperature of 150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

560 - 655 °C

Show Material materials with Melting point of 560 - 655 °C

Typical for Wrought 5000 Series Aluminium

Specific heat capacity

23.0 °C

879 - 963 J/(kg·K)

Show Material materials with Specific heat capacity of 879 - 963 J/(kg·K)

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

23.0 °C

112 - 205 W/(m·K)

Show Material materials with Thermal conductivity of 112 - 205 W/(m·K)

Typical for Wrought 5000 Series Aluminium

Electrical

PropertyTemperatureValueComment

Electrical conductivity

23.0 °C

1.80E+7 - 3.10E+7 S/m

Show Material materials with Electrical conductivity of 1.80E+7 - 3.10E+7 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

23.0 °C

3.3E-8 - 5E-8 Ω·m

Show Material materials with Electrical resistivity of 3.3E-8 - 5E-8 Ω·m

Typical for Wrought 5000 Series Aluminium

Chemical properties

PropertyValue

Iron

0.08 %

Show Material materials with Iron of 0.08 %

Magnesium

0.3 - 0.6 %

Show Material materials with Magnesium of 0.3 - 0.6 %

Manganese

0.03 %

Show Material materials with Manganese of 0.03 %

Other

Mn + Cr = 0.2 - 0.6, Be < 0.0008 for welding additives, each 0.05, total 0.15, Rest Al

Silicon

0.08 %

Show Material materials with Silicon of 0.08 %

Titanium

0.02 %

Show Material materials with Titanium of 0.02 %

Zinc

0.05 %

Show Material materials with Zinc of 0.05 %