AA Standards Grade 1100 H113

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

69 GPa

Show Material materials with Elastic modulus of 69 GPa at 23.0 °C

23.0 °C

Plane-Strain Fracture Toughnes

22 - 35 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23.0 °C

23.0 °C

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C

23.0 °C

Typical for Wrought 1000 Series Aluminium

Shear modulus

25.9 GPa

Show Material materials with Shear modulus of 25.9 GPa at 23.0 °C

23.0 °C

Typical for Wrought 1000 Series Aluminium

Tensile strength

75 MPa

Show Material materials with Tensile strength of 75 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

25 MPa

Show Material materials with Yield strength Rp0.2 of 25 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

2.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.36E-5 1/K at 20.0 °C

20.0 °C

2.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.36E-5 1/K at 100.0 °C

100.0 °C

Melting point

640 - 655 °C

Show Material materials with Melting point of 640 - 655 °C

Specific heat capacity

900 - 963 J/(kg·K)

Show Material materials with Specific heat capacity of 900 - 963 J/(kg·K) at 23.0 °C

23.0 °C

Typical for Wrought 1000 Series Aluminium

Thermal conductivity

218 - 222 W/(m·K)

Show Material materials with Thermal conductivity of 218 - 222 W/(m·K) at 23.0 °C

23.0 °C

Electrical

PropertyValueTemperature

Electrical conductivity

3.30E+7 - 3.40E+7 S/m

Show Material materials with Electrical conductivity of 3.30E+7 - 3.40E+7 S/m at 23.0 °C

23.0 °C

Electrical resistivity

2.94E-8 - 3.03E-8 Ω·m

Show Material materials with Electrical resistivity of 2.94E-8 - 3.03E-8 Ω·m at 23.0 °C

23.0 °C

Chemical properties

Property

Aluminium

99 %

Copper

0.05 - 0.2 %

Manganese

0.05 %

Other

each 0.05, total 0.15, Si + Fe < 0.95

Zinc

0.1 %

Technological properties

Property
Brazing

general: possible with commercial processes and methods

Corrosion properties

Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere

General machinability

General: not suitable (O, H12), poor (H14, H16, H18)

Workability

general (condition): good (O, H12, H14), acceptable (H16), poor(H18)