General
Property | Value | Temperature |
---|---|---|
Density | 2.66 g/cm³ Show Material materials with Density of 2.66 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 70 GPa Show Material materials with Elastic modulus of 70 GPa at 23.0 °C | 23.0 °C | |
Elongation A100 | 10 % Show Material materials with Elongation A100 of 10 % at 23.0 °C | 23.0 °C | |
Elongation A50 | 5 - 12 % Show Material materials with Elongation A50 of 5 - 12 % at 23.0 °C | 23.0 °C | |
Plane-Strain Fracture Toughnes | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Shear modulus | 26 - 26.5 GPa Show Material materials with Shear modulus of 26 - 26.5 GPa at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Tensile strength | 250 - 300 MPa Show Material materials with Tensile strength of 250 - 300 MPa at 23.0 °C | 23.0 °C | |
Yield strength Rp0.2 | 180 MPa Show Material materials with Yield strength Rp0.2 of 180 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 2.39E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.39E-5 1/K at 20.0 °C | 20.0 °C | |
2.39E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.39E-5 1/K at 100.0 °C | 100.0 °C | ||
Max service temperature | 150 °C Show Material materials with Max service temperature of 150 °C | Typical for Wrought 5000 Series Aluminium | |
Melting point | 590 - 645 °C Show Material materials with Melting point of 590 - 645 °C | ||
Specific heat capacity | 879 - 963 J/(kg·K) Show Material materials with Specific heat capacity of 879 - 963 J/(kg·K) at 23.0 °C | 23.0 °C | Typical for Wrought 5000 Series Aluminium |
Thermal conductivity | 126 W/(m·K) Show Material materials with Thermal conductivity of 126 W/(m·K) at 23.0 °C | 23.0 °C |
Electrical
Property | Value | Temperature |
---|---|---|
Electrical conductivity | 1.90E+7 S/m Show Material materials with Electrical conductivity of 1.90E+7 S/m at 23.0 °C | 23.0 °C |
Electrical resistivity | 5.26E-8 Ω·m Show Material materials with Electrical resistivity of 5.26E-8 Ω·m at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Chromium | 0.15 - 0.35 % | |
Copper | 0.05 % | |
Magnesium | 3.1 - 3.9 % | |
Manganese | 0.01 % | |
Other | each 0.05, total 0.15, Rest Al, Si + Fe < 0.45 | |
Titanium | 0.05 % | |
Zinc | 0.2 % |
Technological properties
Property | ||
---|---|---|
Brazing | general: no brazing is known or developed | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: poor (O, H32), sufficient (H34, H36, H38) | |
Workability | general (condition): good (O), acceptable (H32, H34), poor(H36, H38) |