EN 573-3 Grade AW-5454 H28

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlMg alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey,Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

20.0 °C

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

H28

EN 573-3

Flat, Seamless Tube

20.0 °C

2.68 - 2.69 g/cm³

Show Material materials with Density of 2.68 - 2.69 g/cm³

H28

EN 573-3

Flat, Seamless Tube

20.0 °C

2.69 g/cm³

Show Material materials with Density of 2.69 g/cm³

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 573-3

Coil, Sheet, Plate, Flat, Seamless Tube

Dimension

PropertyValueConditionRelated StandardsThicknessShape

Thickness

0.2 mm

Show Material materials with Thickness of 0.2 mm

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

0.2 mm

Coil, Sheet, Plate

3.0 mm

Show Material materials with Thickness of 3.0 mm

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

3.0 mm

Coil, Sheet, Plate

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending Fatigue Strength

145.0 MPa

Show Material materials with Bending Fatigue Strength of 145.0 MPa

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

70.5 GPa

Show Material materials with Elastic modulus of 70.5 GPa

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

20.0 °C

70.5 GPa

Show Material materials with Elastic modulus of 70.5 GPa

H28

EN 573-3

Flat, Seamless Tube

Elongation

3.0 %

Show Material materials with Elongation of 3.0 %

H28

EN 573-3, EN 485

Strip, Sheet, Plate, Rod, Tube

A50

3 %

Show Material materials with Elongation of 3 %

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

A50

3.0 %

Show Material materials with Elongation of 3.0 %

H28

EN 573-3, EN 1592

Strip, Sheet, Plate, Rod, Tube

A100

20.0 °C

3.0 %

Show Material materials with Elongation of 3.0 %

H28

EN 573-3

Flat

A50 Transverse

20.0 °C

3.0 %

Show Material materials with Elongation of 3.0 %

H28

EN 573-3

Seamless Tube

20.0 °C

3.0 %

Show Material materials with Elongation of 3.0 %

H28

EN 573-3

Flat

A50

Hardness, Brinell

93.0 [-]

Show Material materials with Hardness, Brinell of 93.0 [-]

H28

EN 573-3, EN 485

Strip, Sheet, Plate, Rod, Tube

20.0 °C

93.0 [-]

Show Material materials with Hardness, Brinell of 93.0 [-]

H28

EN 573-3

Flat

Hardness, HBW

93 [-]

Show Material materials with Hardness, HBW of 93 [-]

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

20.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

H28

EN 573-3

Flat, Seamless Tube

Shear modulus

26.5 GPa

Show Material materials with Shear modulus of 26.5 GPa

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

26.6 GPa

Show Material materials with Shear modulus of 26.6 GPa

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

20.0 °C

26.5 - 27.0 GPa

Show Material materials with Shear modulus of 26.5 - 27.0 GPa

H28

EN 573-3

Flat, Seamless Tube

20.0 °C

26.5 GPa

Show Material materials with Shear modulus of 26.5 GPa

H28

EN 573-3

Flat, Seamless Tube

Tensile strength

310.0 MPa

Show Material materials with Tensile strength of 310.0 MPa

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

310 MPa

Show Material materials with Tensile strength of 310 MPa

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

20.0 °C

310.0 MPa

Show Material materials with Tensile strength of 310.0 MPa

H28

EN 573-3

Flat

Transverse

20.0 °C

310.0 MPa

Show Material materials with Tensile strength of 310.0 MPa

H28

EN 573-3

Seamless Tube, Flat

Yield strength

250.0 MPa

Show Material materials with Yield strength of 250.0 MPa

H28

EN 573-3, EN 485

Strip, Sheet, Plate, Rod, Tube

RP02

250 MPa

Show Material materials with Yield strength of 250 MPa

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

280.0 MPa

Show Material materials with Yield strength of 280.0 MPa

H28

EN 573-3, EN 1592

Strip, Sheet, Plate, Rod, Tube

RP02

20.0 °C

250.0 MPa

Show Material materials with Yield strength of 250.0 MPa

H28

EN 573-3

Flat

RP02 Transverse

20.0 °C

250.0 MPa

Show Material materials with Yield strength of 250.0 MPa

H28

EN 573-3

Flat

RP02

20.0 °C

280.0 MPa

Show Material materials with Yield strength of 280.0 MPa

H28

EN 573-3

Seamless Tube

RP02

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

-50 °C

2.1899999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1899999999999997e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

-50.0 °C

2.19e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.19e-05 1/K

H28

EN 573-3

Flat, Seamless Tube

20 °C

2.1899999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1899999999999997e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

20 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

20 °C

2.46e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.46e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube, Flat, Seamless Tube

20 °C

2.56e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.56e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube, Flat, Seamless Tube

100 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

100.0 °C

2.37e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.37e-05 1/K

H28

EN 573-3

Flat, Seamless Tube

100 °C

0.000024 1/K

Show Material materials with Coefficient of thermal expansion of 0.000024 1/K

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

20-100°C

200 °C

2.46e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.46e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube, Flat, Seamless Tube

200.0 °C

2.46e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.46e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube, Flat, Seamless Tube

300 °C

2.56e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.56e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube, Flat, Seamless Tube

300.0 °C

2.56e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.56e-05 1/K

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube, Flat, Seamless Tube

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

602.0 - 646.0 °C

Show Material materials with Melting point of 602.0 - 646.0 °C

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

20.0 °C

897.0 - 900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 897.0 - 900.0 J/(kg·K)

H28

EN 573-3

Flat, Seamless Tube

20.0 °C

897.0 J/(kg·K)

Show Material materials with Specific heat capacity of 897.0 J/(kg·K)

H28

EN 573-3

Flat, Seamless Tube

20.0 °C

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H28

EN 573-3

Flat, Seamless Tube

Thermal conductivity

130.0 - 150.0 W/(m·K)

Show Material materials with Thermal conductivity of 130.0 - 150.0 W/(m·K)

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

134 W/(m·K)

Show Material materials with Thermal conductivity of 134 W/(m·K)

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

20.0 °C

135.0 - 150.0 W/(m·K)

Show Material materials with Thermal conductivity of 135.0 - 150.0 W/(m·K)

H28

EN 573-3

Flat, Seamless Tube

20.0 °C

135.0 W/(m·K)

Show Material materials with Thermal conductivity of 135.0 W/(m·K)

H28

EN 573-3

Flat, Seamless Tube

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

19000000.0 - 21000000.0 S/m

Show Material materials with Electrical conductivity of 19000000.0 - 21000000.0 S/m

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

20.0 °C

21000000.0 S/m

Show Material materials with Electrical conductivity of 21000000.0 S/m

H28

EN 573-3

Flat, Seamless Tube

Electrical resistivity

4.76e-08 - 5.26e-08 Ω·m

Show Material materials with Electrical resistivity of 4.76e-08 - 5.26e-08 Ω·m

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

20.0 °C

5.1e-08 Ω·m

Show Material materials with Electrical resistivity of 5.1e-08 Ω·m

H28

EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2

Flat, Seamless Tube, Coil, Sheet, Plate

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.05 - 0.2 %

Show Material materials with Chromium of 0.05 - 0.2 %

H28

EN 573-3, EN 1592, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2

Flat, Seamless Tube, Strip, Sheet, Plate, Rod, Tube, Coil, Sheet, Plate

Copper

0.1 %

Show Material materials with Copper of 0.1 %

H28

EN 573-3, EN 1592, EN 485

Flat, Seamless Tube, Strip, Sheet, Plate, Rod, Tube

0.1 %

Show Material materials with Copper of 0.1 %

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

Iron

0.4 %

Show Material materials with Iron of 0.4 %

H28

EN 573-3

Flat, Seamless Tube

0.40 %

Show Material materials with Iron of 0.40 %

H28

EN 573-3, EN 1592, EN 485

Strip, Sheet, Plate, Rod, Tube

0.4 %

Show Material materials with Iron of 0.4 %

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

Magnesium

2.4 - 3.0 %

Show Material materials with Magnesium of 2.4 - 3.0 %

H28

EN 573-3, EN 1592, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2

Flat, Seamless Tube, Strip, Sheet, Plate, Rod, Tube, Coil, Sheet, Plate

Manganese

0.5 - 1.0 %

Show Material materials with Manganese of 0.5 - 1.0 %

H28

EN 573-3, EN 1592, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2

Flat, Seamless Tube, Strip, Sheet, Plate, Rod, Tube, Coil, Sheet, Plate

Other

0.05 - 0.15 %

Show Material materials with Other of 0.05 - 0.15 %

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

Silicon

0.25 %

Show Material materials with Silicon of 0.25 %

H28

EN 573-3, EN 1592, EN 485

Flat, Seamless Tube, Strip, Sheet, Plate, Rod, Tube

0.25 %

Show Material materials with Silicon of 0.25 %

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

Titanium

0.2 %

Show Material materials with Titanium of 0.2 %

H28

EN 573-3, EN 1592, EN 485

Flat, Seamless Tube, Strip, Sheet, Plate, Rod, Tube

0.2 %

Show Material materials with Titanium of 0.2 %

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

H28

EN 573-3, EN 1592, EN 485

Flat, Seamless Tube, Strip, Sheet, Plate, Rod, Tube

0.25 %

Show Material materials with Zinc of 0.25 %

H28

EN 573-1, EN 573-2, EN 573-3, EN 485-2

Coil, Sheet, Plate

Technological properties

Property
Anodizing

decorative: sufficient, Protective: good

Application areas

Vessels: Pressure; Components: General transportation

Brazing

hard brazing (with flux/ without flux): poor / sufficient, friction soldering: acceptable, soft brazing with flux: poor

Corrosion properties

Seawater: very good, weathering: very good

General machinability

Fair

Surface Finish

Mill finish.

Welding

Very Good

Workability

Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): sufficient, Deep drawing / upsetting (Condition) good (O) / good (H12)