EN 573-3 Grade AW-6008 T6

Want to keep this datasheet? Save it now in your required format

Description

Age-hardenable AlMgSi alloy. The alloy is not food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

T6

EN 573-3, EN 13981-1, EN 755

Rod, Tube

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

Typical for Wrought 6000 Series Aluminium

Elongation

6.0 %

Show Material materials with Elongation of 6.0 %

T6

EN 573-3, EN 13981-1, EN 755

Rod, Tube

A50

8.0 %

Show Material materials with Elongation of 8.0 %

T6

EN 573-3, EN 13981-1, EN 755

Rod, Tube

A100

20.0 °C

6.0 %

Show Material materials with Elongation of 6.0 %

T6

EN 573-3

Profile, Tube

A50

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

T6

EN 573-3

Profile, Tube

Hardness, Brinell

85.0 [-]

Show Material materials with Hardness, Brinell of 85.0 [-]

T6

EN 573-3, EN 755

Rod, Tube

90.0 [-]

Show Material materials with Hardness, Brinell of 90.0 [-]

T6

EN 573-3, EN 755

Rod, Tube

20.0 °C

85.0 [-]

Show Material materials with Hardness, Brinell of 85.0 [-]

T6

EN 573-3

Profile, Tube

20.0 °C

85.0 - 90.0 [-]

Show Material materials with Hardness, Brinell of 85.0 - 90.0 [-]

T6

EN 573-3

Profile, Tube

20.0 °C

90.0 [-]

Show Material materials with Hardness, Brinell of 90.0 [-]

T6

EN 573-3

Profile, Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 6000 Series Aluminium

Tensile strength

250.0 MPa

Show Material materials with Tensile strength of 250.0 MPa

T6

EN 573-3, EN 13981-1

Rod, Tube

255.0 MPa

Show Material materials with Tensile strength of 255.0 MPa

T6

EN 573-3, EN 13981-1

Rod, Tube

260.0 MPa

Show Material materials with Tensile strength of 260.0 MPa

T6

EN 573-3, EN 13981-1, EN 755

Rod, Tube

270.0 MPa

Show Material materials with Tensile strength of 270.0 MPa

T6

EN 573-3, EN 13981-1, EN 755

Rod, Tube

20.0 °C

250.0 MPa

Show Material materials with Tensile strength of 250.0 MPa

T6

EN 573-3

Profile

20.0 °C

255.0 MPa

Show Material materials with Tensile strength of 255.0 MPa

T6

EN 573-3

Profile

20.0 °C

260.0 MPa

Show Material materials with Tensile strength of 260.0 MPa

T6

EN 573-3

Profile, Tube

20.0 °C

270.0 MPa

Show Material materials with Tensile strength of 270.0 MPa

T6

EN 573-3

Profile, Tube

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.6e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.4e-05 1/K

Typical for Wrought 6000 Series Aluminium

Melting point

555.0 - 655.0 °C

Show Material materials with Melting point of 555.0 - 655.0 °C

Typical for Wrought 6000 Series Aluminium

Specific heat capacity

887.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Thermal conductivity

170.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 170.0 - 220.0 W/(m·K)

Typical for Wrought 6000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

21000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 21000000.0 - 34000000.0 S/m

Typical for Wrought 6000 Series Aluminium

Electrical resistivity

2.9e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 2.9e-08 - 5e-08 Ω·m

Typical for Wrought 6000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Copper

0.3 %

Show Material materials with Copper of 0.3 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Iron

0.35 %

Show Material materials with Iron of 0.35 %

T6

EN 573-3

Profile, Tube

0.35 %

Show Material materials with Iron of 0.35 %

T6

EN 573-3, EN 13981-1, EN 755

Rod, Tube

Magnesium

0.4 - 0.7 %

Show Material materials with Magnesium of 0.4 - 0.7 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Manganese

0.3 %

Show Material materials with Manganese of 0.3 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Silicon

0.5 - 0.9 %

Show Material materials with Silicon of 0.5 - 0.9 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Vanadium

0.05 - 0.2 %

Show Material materials with Vanadium of 0.05 - 0.2 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

T6

EN 573-3, EN 13981-1, EN 755

Profile, Tube, Rod

Technological properties

Property
Workability

Excellent workability.