General
Property | Value | Condition | Related Standards |
---|---|---|---|
Density | 2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ | T6 | AA Standards, ASTM B221 |
Mechanical
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Bending Fatigue Strength | 70.0 MPa Show Material materials with Bending Fatigue Strength of 70.0 MPa | T6 | AA Standards | |
Elastic modulus | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | T6 | AA Standards, ASTM B221 | |
Hardness, Brinell | 74.0 [-] Show Material materials with Hardness, Brinell of 74.0 [-] | T6 | AA Standards | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||
Shear modulus | 26.0 - 26.5 GPa Show Material materials with Shear modulus of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||
Tensile strength | 205.0 MPa Show Material materials with Tensile strength of 205.0 MPa | T6 | AA Standards, ASTM B221 | |
240.0 MPa Show Material materials with Tensile strength of 240.0 MPa | T6 | AA Standards |
Thermal
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.3399999999999996e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K | T6 | AA Standards, ASTM B221 | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K | T6 | AA Standards, ASTM B221 | ||
Melting point | 615.0 - 655.0 °C Show Material materials with Melting point of 615.0 - 655.0 °C | T6 | AA Standards, ASTM B221 | ||
Specific heat capacity | 887.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | |||
Thermal conductivity | 193.0 - 209.0 W/(m·K) Show Material materials with Thermal conductivity of 193.0 - 209.0 W/(m·K) | T6 | AA Standards, ASTM B221 |
Electrical
Property | Value | Condition | Related Standards |
---|---|---|---|
Electrical conductivity | 29000000.0 - 32000000.0 S/m Show Material materials with Electrical conductivity of 29000000.0 - 32000000.0 S/m | T6 | AA Standards, ASTM B221 |
Electrical resistivity | 3.13e-08 - 3.45e-08 Ω·m Show Material materials with Electrical resistivity of 3.13e-08 - 3.45e-08 Ω·m | T6 | AA Standards, ASTM B221 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Copper | 0.2 % Show Material materials with Copper of 0.2 % | T6 | AA Standards, ASTM B221 |
Iron | 0.15 % Show Material materials with Iron of 0.15 % | T6 | AA Standards, ASTM B221 |
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % | T6 | AA Standards, ASTM B221 |
Manganese | 0.05 % Show Material materials with Manganese of 0.05 % | T6 | AA Standards, ASTM B221 |
Silicon | 0.2 - 0.6 % Show Material materials with Silicon of 0.2 - 0.6 % | T6 | AA Standards, ASTM B221 |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | T6 | AA Standards, ASTM B221 |
Technological properties
Property | ||
---|---|---|
Brazing | general: possible with commercial processes and methods | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: poor (T1), sufficient (T5, T6) | |
Workability | general (condition): acceptable (T1, T5), poor(T6) |