General
Property | Value | Related Standards |
---|---|---|
Density | 2.82 g/cm³ Show Material materials with Density of 2.82 g/cm³ | AA Standards |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 69.0 - 72.0 GPa Show Material materials with Elastic modulus of 69.0 - 72.0 GPa | Typical for Wrought 7000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 7000 Series Aluminium |
Shear modulus | 26.4 - 27.1 GPa Show Material materials with Shear modulus of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Melting point | 465.0 - 655.0 °C Show Material materials with Melting point of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Specific heat capacity | 795.0 - 1050.0 J/(kg·K) Show Material materials with Specific heat capacity of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Thermal conductivity | 121.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 18000000.0 - 34000000.0 S/m Show Material materials with Electrical conductivity of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
Electrical resistivity | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Electrical resistivity of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Bismuth | 0.01 % Show Material materials with Bismuth of 0.01 % | AA Standards |
Chromium | 0.15 - 0.25 % Show Material materials with Chromium of 0.15 - 0.25 % | AA Standards |
Copper | 1.7 - 2.3 % Show Material materials with Copper of 1.7 - 2.3 % | AA Standards |
Iron | 0.12 % Show Material materials with Iron of 0.12 % | AA Standards |
Lead | 0.01 % Show Material materials with Lead of 0.01 % | AA Standards |
Magnesium | 1.5 - 2.5 % Show Material materials with Magnesium of 1.5 - 2.5 % | AA Standards |
Manganese | 0.05 % Show Material materials with Manganese of 0.05 % | AA Standards |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % | AA Standards |
Titanium | 0.1 % Show Material materials with Titanium of 0.1 % | AA Standards |
Zinc | 5.5 - 6.5 % Show Material materials with Zinc of 5.5 - 6.5 % | AA Standards |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |