AA Standards Grade 6061 O

View suppliers (225)
Want to keep this datasheet? Save it now in your required format

Description

AA 6061 is a readily available alloy that has good surface finish and ability to be anodized.Easy of weldability and brazability with nice surface finish. Resistance to corrosion from seawater and atmospheric conditions. Suitable for hot forging.

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated Standards

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Mechanical

PropertyValueConditionRelated StandardsComment

Bending Fatigue Strength

60.0 MPa

Show Material materials with Bending Fatigue Strength of 60.0 MPa

O

AA Standards

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Hardness, Brinell

30.0 [-]

Show Material materials with Hardness, Brinell of 30.0 [-]

O

AA Standards

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 6000 Series Aluminium

Tensile strength

125.0 MPa

Show Material materials with Tensile strength of 125.0 MPa

O

AA Standards

150.0 MPa

Show Material materials with Tensile strength of 150.0 MPa

O

AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B313, ASTM B345, ASTM B483

155.0 MPa

Show Material materials with Tensile strength of 155.0 MPa

O

AA Standards, ASTM B211, ASTM B316

Thermal

PropertyTemperatureValueConditionRelated StandardsComment

Coefficient of thermal expansion

20 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

100 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Melting point

580.0 - 650.0 °C

Show Material materials with Melting point of 580.0 - 650.0 °C

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Specific heat capacity

887.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Thermal conductivity

155.0 - 180.0 W/(m·K)

Show Material materials with Thermal conductivity of 155.0 - 180.0 W/(m·K)

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Electrical

PropertyValueConditionRelated Standards

Electrical conductivity

23000000.0 - 27000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 27000000.0 S/m

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Electrical resistivity

3.7e-08 - 4.35e-08 Ω·m

Show Material materials with Electrical resistivity of 3.7e-08 - 4.35e-08 Ω·m

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Chemical properties

PropertyValueConditionRelated Standards

Chromium

0.04 - 0.35 %

Show Material materials with Chromium of 0.04 - 0.35 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Copper

0.15 - 0.4 %

Show Material materials with Copper of 0.15 - 0.4 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Iron

0.70 %

Show Material materials with Iron of 0.70 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Magnesium

0.8 - 1.2 %

Show Material materials with Magnesium of 0.8 - 1.2 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Manganese

0.15 %

Show Material materials with Manganese of 0.15 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Silicon

0.4 - 0.8 %

Show Material materials with Silicon of 0.4 - 0.8 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

O

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B313, ASTM B316, ASTM B345, ASTM B483

Technological properties

Property
Brazing

general: possible with commercial processes and methods

Corrosion properties

Stress corrosion cracking: no damage during operation and laboratory tests (O, T6, T651, T652, T6510, T6511), no damage during operation, limited damage during laboratory tests (T4, T451, T4510, T4511), general: good, without protection in industrial or seawater atmosphere

General machinability

General: poor (O), sufficient (T4, T451, T4510, T4511, T6, T651, T652, T6510, T6511)

Workability

general (condition): good (O), acceptable (T4, T451, T4510, T4511), poor(T6, T651, T652, T6510, T6511)