EN 573-3 Grade AW-6063 T66

Want to keep this datasheet? Save it now in your required format

Description

Aluminum EN AW-6063 is an architectural alloy that offers users a high resistance to corrosion and excellent finishing characteristics. Easy to extrude with fair machinability, EN AW-6063 can be both hot and cold formed and is commonly available as T6 temper as well as T4 temper.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

69.5 GPa

Show Material materials with Elastic modulus of 69.5 GPa

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Elongation

6.0 %

Show Material materials with Elongation of 6.0 %

T66

EN 573-3, EN 12020, EN 755

Strip, Sheet, Plate, Tube, Bar

A50

8.0 %

Show Material materials with Elongation of 8.0 %

T66

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

A50

8.0 %

Show Material materials with Elongation of 8.0 %

T66

EN 573-3, EN 12020, EN 755

Strip, Sheet, Plate, Tube, Bar

A100

10.0 %

Show Material materials with Elongation of 10.0 %

T66

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

A100

20.0 °C

6.0 %

Show Material materials with Elongation of 6.0 %

T66

EN 573-3

Profile

A50

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

T66

EN 573-3

Rod, Tube

A50

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

T66

EN 573-3

Profile

20.0 °C

10.0 %

Show Material materials with Elongation of 10.0 %

T66

EN 573-3

Profile

A50

20.0 °C

10.0 %

Show Material materials with Elongation of 10.0 %

T66

EN 573-3

Rod, Tube

20.0 °C

12.0 %

Show Material materials with Elongation of 12.0 %

T66

EN 573-3

Profile

Hardness, Brinell

20.0 °C

80.0 [-]

Show Material materials with Hardness, Brinell of 80.0 [-]

T66

EN 573-3

Profile, Rod, Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

26.1 GPa

Show Material materials with Shear modulus of 26.1 GPa

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Tensile strength

225.0 MPa

Show Material materials with Tensile strength of 225.0 MPa

T66

EN 573-3, EN 12020, EN 755

Strip, Sheet, Plate, Tube, Bar

230.0 MPa

Show Material materials with Tensile strength of 230.0 MPa

T66

EN 573-3, EN 754

Strip, Sheet, Plate, Tube, Bar

245.0 MPa

Show Material materials with Tensile strength of 245.0 MPa

T66

EN 573-3, EN 12020, EN 755

Strip, Sheet, Plate, Tube, Bar

20.0 °C

180.0 MPa

Show Material materials with Tensile strength of 180.0 MPa

T66

EN 573-3

Profile

20.0 °C

225.0 MPa

Show Material materials with Tensile strength of 225.0 MPa

T66

EN 573-3

Profile

20.0 °C

230.0 MPa

Show Material materials with Tensile strength of 230.0 MPa

T66

EN 573-3

Rod, Tube

20.0 °C

245.0 MPa

Show Material materials with Tensile strength of 245.0 MPa

T66

EN 573-3

Rod, Tube, Profile

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.3399999999999996e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

100 °C

2.3399999999999996e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Melting point

615.0 - 655.0 °C

Show Material materials with Melting point of 615.0 - 655.0 °C

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Specific heat capacity

887.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Thermal conductivity

193.0 - 218.0 W/(m·K)

Show Material materials with Thermal conductivity of 193.0 - 218.0 W/(m·K)

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Electrical

PropertyValueConditionRelated StandardsShape

Electrical conductivity

29000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 29000000.0 - 34000000.0 S/m

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Electrical resistivity

2.94e-08 - 3.45e-08 Ω·m

Show Material materials with Electrical resistivity of 2.94e-08 - 3.45e-08 Ω·m

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Copper

0.1 %

Show Material materials with Copper of 0.1 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Iron

0.35 %

Show Material materials with Iron of 0.35 %

T66

EN 573-3

Profile, Rod, Tube

0.35 %

Show Material materials with Iron of 0.35 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Strip, Sheet, Plate, Tube, Bar

Magnesium

0.45 - 0.9 %

Show Material materials with Magnesium of 0.45 - 0.9 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Silicon

0.2 - 0.6 %

Show Material materials with Silicon of 0.2 - 0.6 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

T66

EN 573-3, EN 12020, EN 13195, EN 754, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Technological properties

Property
Anodizing

decorative: acceptable, Protective: very good

Brazing

hard brazing (with flux/ without flux): acceptable to poor / sufficient, friction soldering: good, soft brazing with flux: acceptable

Corrosion properties

Seawater: good to acceptable, weathering: good

Workability

Excellent workability.