EN 573-3 Grade AW-6101 T1

Want to keep this datasheet? Save it now in your required format

Description

EN AW-6101 is an alloy that offers users a high electrical conductivity and good mechanical strength. Standard methods can be used to machine, weld, and form Aluminum EN AW-6101 and it is easily extruded. EN AW-6101 also offers good corrosion resistance, bendability, and formability. Unlike other aluminum alloys, EN AW-6101 can be both hot and cold worked.

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

T1

EN 573-3, EN 1715-2

Wire

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

T1

EN 573-3, EN 1715-2

Wire

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 6000 Series Aluminium

Tensile strength

190.0 MPa

Show Material materials with Tensile strength of 190.0 MPa

T1

EN 573-3, EN 1715-2

Wire

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

100 °C, 20 °C

2.3399999999999996e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K

T1

EN 573-3, EN 1715-2

Wire

Melting point

620.0 - 655.0 °C

Show Material materials with Melting point of 620.0 - 655.0 °C

T1

EN 573-3, EN 1715-2

Wire

Specific heat capacity

887.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Thermal conductivity

218.0 - 226.0 W/(m·K)

Show Material materials with Thermal conductivity of 218.0 - 226.0 W/(m·K)

T1

EN 573-3, EN 1715-2

Wire

Electrical

PropertyValueConditionRelated StandardsShape

Electrical conductivity

33000000.0 - 35000000.0 S/m

Show Material materials with Electrical conductivity of 33000000.0 - 35000000.0 S/m

T1

EN 573-3, EN 1715-2

Wire

Electrical resistivity

2.86e-08 - 3.03e-08 Ω·m

Show Material materials with Electrical resistivity of 2.86e-08 - 3.03e-08 Ω·m

T1

EN 573-3, EN 1715-2

Wire

Chemical properties

PropertyValueConditionRelated StandardsShape

Boron

0.06 %

Show Material materials with Boron of 0.06 %

T1

EN 573-3, EN 1715-2

Wire

Chromium

0.03 %

Show Material materials with Chromium of 0.03 %

T1

EN 573-3, EN 1715-2

Wire

Copper

0.1 %

Show Material materials with Copper of 0.1 %

T1

EN 573-3, EN 1715-2

Wire

Iron

0.50 %

Show Material materials with Iron of 0.50 %

T1

EN 573-3, EN 1715-2

Wire

Magnesium

0.35 - 0.8 %

Show Material materials with Magnesium of 0.35 - 0.8 %

T1

EN 573-3, EN 1715-2

Wire

Manganese

0.03 %

Show Material materials with Manganese of 0.03 %

T1

EN 573-3, EN 1715-2

Wire

Silicon

0.3 - 0.7 %

Show Material materials with Silicon of 0.3 - 0.7 %

T1

EN 573-3, EN 1715-2

Wire

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

T1

EN 573-3, EN 1715-2

Wire

Technological properties

Property
Workability

Excellent workability.