EN 573-3 Grade AW-6951 O

Want to keep this datasheet? Save it now in your required format

Description

Age-hardenable AlMgSi alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

O

EN 573-3, EN 683

Strip, Sheet

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

Typical for Wrought 6000 Series Aluminium

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 6000 Series Aluminium

Tensile strength

20.0 °C

80.0 - 140.0 MPa

Show Material materials with Tensile strength of 80.0 - 140.0 MPa

O

EN 573-3, EN 683

Strip, Sheet, Foil

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.3399999999999996e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K

O

EN 573-3, EN 683

Strip, Sheet

100 °C

2.3399999999999996e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K

O

EN 573-3, EN 683

Strip, Sheet

Melting point

615.0 - 655.0 °C

Show Material materials with Melting point of 615.0 - 655.0 °C

O

EN 573-3, EN 683

Strip, Sheet

Specific heat capacity

887.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Thermal conductivity

197.0 - 213.0 W/(m·K)

Show Material materials with Thermal conductivity of 197.0 - 213.0 W/(m·K)

O

EN 573-3, EN 683

Strip, Sheet

213.0 W/(m·K)

Show Material materials with Thermal conductivity of 213.0 W/(m·K)

O

EN 573-3, EN 683

Strip, Sheet

Electrical

PropertyValueConditionRelated StandardsShape

Electrical conductivity

30000000.0 - 32000000.0 S/m

Show Material materials with Electrical conductivity of 30000000.0 - 32000000.0 S/m

O

EN 573-3, EN 683

Strip, Sheet

32000000.0 S/m

Show Material materials with Electrical conductivity of 32000000.0 S/m

O

EN 573-3, EN 683

Strip, Sheet

Electrical resistivity

3.13e-08 - 3.33e-08 Ω·m

Show Material materials with Electrical resistivity of 3.13e-08 - 3.33e-08 Ω·m

O

EN 573-3, EN 683

Strip, Sheet

3.13e-08 Ω·m

Show Material materials with Electrical resistivity of 3.13e-08 Ω·m

O

EN 573-3, EN 683

Strip, Sheet

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.15 - 0.4 %

Show Material materials with Copper of 0.15 - 0.4 %

O

EN 573-3, EN 683

Foil, Strip, Sheet

Iron

0.8 %

Show Material materials with Iron of 0.8 %

O

EN 573-3

Foil

0.80 %

Show Material materials with Iron of 0.80 %

O

EN 573-3, EN 683

Strip, Sheet

Magnesium

0.4 - 0.8 %

Show Material materials with Magnesium of 0.4 - 0.8 %

O

EN 573-3, EN 683

Foil, Strip, Sheet

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

O

EN 573-3, EN 683

Foil, Strip, Sheet

Silicon

0.2 - 0.5 %

Show Material materials with Silicon of 0.2 - 0.5 %

O

EN 573-3, EN 683

Foil, Strip, Sheet

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

O

EN 573-3, EN 683

Foil, Strip, Sheet

Technological properties

Property
Workability

Excellent workability.