General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Density | 2.77 g/cm³ Show Material materials with Density of 2.77 g/cm³ | T6 | EN 573-3, EN 755 | Rod, Tube |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 69.0 - 72.0 GPa Show Material materials with Elastic modulus of 69.0 - 72.0 GPa | Typical for Wrought 7000 Series Aluminium | ||||
Elongation | 8.0 % Show Material materials with Elongation of 8.0 % | T6 | EN 573-3, EN 755 | Rod, Tube | A50 | |
10.0 % Show Material materials with Elongation of 10.0 % | T6 | EN 573-3, EN 755 | Rod, Tube | A100 | ||
20.0 °C | 8.0 % Show Material materials with Elongation of 8.0 % | T6 | EN 573-3 | Profile, Rod, Tube | A50 | |
20.0 °C | 10.0 % Show Material materials with Elongation of 10.0 % | T6 | EN 573-3 | Profile, Tube, Rod | ||
Hardness, Brinell | 20.0 °C | 110.0 [-] Show Material materials with Hardness, Brinell of 110.0 [-] | T6 | EN 573-3 | Profile, Rod, Tube | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Shear modulus | 26.4 - 27.1 GPa Show Material materials with Shear modulus of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium | ||||
Tensile strength | 340.0 MPa Show Material materials with Tensile strength of 340.0 MPa | T6 | EN 573-3, EN 755 | Rod, Tube | ||
350.0 MPa Show Material materials with Tensile strength of 350.0 MPa | T6 | EN 573-3, EN 755 | Rod, Tube | |||
20.0 °C | 340.0 MPa Show Material materials with Tensile strength of 340.0 MPa | T6 | EN 573-3 | Rod | ||
20.0 °C | 350.0 MPa Show Material materials with Tensile strength of 350.0 MPa | T6 | EN 573-3 | Profile, Tube, Rod |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Melting point | 465.0 - 655.0 °C Show Material materials with Melting point of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Specific heat capacity | 795.0 - 1050.0 J/(kg·K) Show Material materials with Specific heat capacity of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Thermal conductivity | 121.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 18000000.0 - 34000000.0 S/m Show Material materials with Electrical conductivity of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
Electrical resistivity | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Electrical resistivity of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.06 - 0.2 % Show Material materials with Chromium of 0.06 - 0.2 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Copper | 0.1 % Show Material materials with Copper of 0.1 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Iron | 0.4 % Show Material materials with Iron of 0.4 % | T6 | EN 573-3 | Profile, Rod, Tube |
0.40 % Show Material materials with Iron of 0.40 % | T6 | EN 573-3, EN 755 | Rod, Tube | |
Magnesium | 1.0 - 1.8 % Show Material materials with Magnesium of 1.0 - 1.8 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Manganese | 0.2 - 0.7 % Show Material materials with Manganese of 0.2 - 0.7 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Silicon | 0.35 % Show Material materials with Silicon of 0.35 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Titanium | 0.01 - 0.06 % Show Material materials with Titanium of 0.01 - 0.06 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Zinc | 4.0 - 5.0 % Show Material materials with Zinc of 4.0 - 5.0 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Zirconium | 0.08 - 0.2 % Show Material materials with Zirconium of 0.08 - 0.2 % | T6 | EN 573-3, EN 755 | Profile, Rod, Tube |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |