EN 573-3 Grade AW-7021 T6

Want to keep this datasheet? Save it now in your required format

Description

Age-hardenable AlZn alloy. The alloy is not food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.78 g/cm³

Show Material materials with Density of 2.78 g/cm³

T6

EN 573-3, EN 485, EN 755

Strip, Sheet, Plate, Rod, Tube, Welded Tube

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 - 72.0 GPa

Show Material materials with Elastic modulus of 69.0 - 72.0 GPa

Typical for Wrought 7000 Series Aluminium

Elongation

7.0 %

Show Material materials with Elongation of 7.0 %

T6

EN 573-3, EN 485

Strip, Sheet, Plate, Rod, Tube, Welded Tube

A50

8.0 %

Show Material materials with Elongation of 8.0 %

T6

EN 573-3, EN 485, EN 755

Strip, Sheet, Plate, Rod, Tube, Welded Tube

A50

10.0 %

Show Material materials with Elongation of 10.0 %

T6

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Tube, Welded Tube

A100

20.0 °C

7.0 %

Show Material materials with Elongation of 7.0 %

T6

EN 573-3

Flat

A50

20.0 °C

7.0 %

Show Material materials with Elongation of 7.0 %

T6

EN 573-3

Flat

A50 Transverse

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

T6

EN 573-3

Profile, Rod, Tube, Flat

A50

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

T6

EN 573-3

Flat

A50 Transverse

20.0 °C

10.0 %

Show Material materials with Elongation of 10.0 %

T6

EN 573-3

Profile, Rod, Tube

Hardness, Brinell

120.0 [-]

Show Material materials with Hardness, Brinell of 120.0 [-]

T6

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Tube, Welded Tube

121.0 [-]

Show Material materials with Hardness, Brinell of 121.0 [-]

T6

EN 573-3, EN 485

Strip, Sheet, Plate, Rod, Tube, Welded Tube

20.0 °C

120.0 [-]

Show Material materials with Hardness, Brinell of 120.0 [-]

T6

EN 573-3

Profile, Rod, Tube

20.0 °C

121.0 [-]

Show Material materials with Hardness, Brinell of 121.0 [-]

T6

EN 573-3

Flat

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 7000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 7000 Series Aluminium

Shear modulus

26.4 - 27.1 GPa

Show Material materials with Shear modulus of 26.4 - 27.1 GPa

Typical for Wrought 7000 Series Aluminium

Tensile strength

400.0 MPa

Show Material materials with Tensile strength of 400.0 MPa

T6

EN 573-3, EN 485

Strip, Sheet, Plate, Rod, Tube, Welded Tube

410.0 MPa

Show Material materials with Tensile strength of 410.0 MPa

T6

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Tube, Welded Tube

20.0 °C

400.0 MPa

Show Material materials with Tensile strength of 400.0 MPa

T6

EN 573-3

Flat

20.0 °C

400.0 MPa

Show Material materials with Tensile strength of 400.0 MPa

T6

EN 573-3

Flat

Transverse

20.0 °C

410.0 MPa

Show Material materials with Tensile strength of 410.0 MPa

T6

EN 573-3

Profile, Rod, Tube

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.1e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1e-05 - 2.4e-05 1/K

Typical for Wrought 7000 Series Aluminium

Melting point

465.0 - 655.0 °C

Show Material materials with Melting point of 465.0 - 655.0 °C

Typical for Wrought 7000 Series Aluminium

Specific heat capacity

795.0 - 1050.0 J/(kg·K)

Show Material materials with Specific heat capacity of 795.0 - 1050.0 J/(kg·K)

Typical for Wrought 7000 Series Aluminium

Thermal conductivity

121.0 - 170.0 W/(m·K)

Show Material materials with Thermal conductivity of 121.0 - 170.0 W/(m·K)

Typical for Wrought 7000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 34000000.0 S/m

Typical for Wrought 7000 Series Aluminium

Electrical resistivity

2.9e-08 - 5.6e-08 Ω·m

Show Material materials with Electrical resistivity of 2.9e-08 - 5.6e-08 Ω·m

Typical for Wrought 7000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.05 %

Show Material materials with Chromium of 0.05 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Copper

0.25 %

Show Material materials with Copper of 0.25 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Iron

0.4 %

Show Material materials with Iron of 0.4 %

T6

EN 573-3

Profile, Rod, Flat, Tube

0.40 %

Show Material materials with Iron of 0.40 %

T6

EN 573-3, EN 485, EN 755

Strip, Sheet, Plate, Rod, Tube, Welded Tube

Magnesium

1.2 - 1.8 %

Show Material materials with Magnesium of 1.2 - 1.8 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Silicon

0.25 %

Show Material materials with Silicon of 0.25 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Zinc

5.0 - 6.0 %

Show Material materials with Zinc of 5.0 - 6.0 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Zirconium

0.08 - 0.18 %

Show Material materials with Zirconium of 0.08 - 0.18 %

T6

EN 573-3, EN 485, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube

Technological properties

Property
Brazing

Excellent