Properties

General

Density

ρ

2.69 - 2.7 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.2 - 3 mm

Mechanical

Elastic modulus

E

70 GPa at -270 °C

Show 1000 Series materials with Elastic modulus of 70 GPa at -270 °C

Hide chart

Elongation A100

A100

1 % at 20 °C

Show 1000 Series materials with Elongation A100 of 1 % at 20 °C

Elongation A50

A50

1 % at 20 °C

Show 1000 Series materials with Elongation A50 of 1 % at 20 °C

Elongation A50, transverse

A50,trans

1 % at 20 °C

Show 1000 Series materials with Elongation A50, transverse of 1 % at 20 °C

Hardness, Brinell

HB

45 [-] at 20 °C

Show 1000 Series materials with Hardness, Brinell of 45 [-] at 20 °C

Hardness, HBW

HBW

45 [-] at 20 °C

Show 1000 Series materials with Hardness, HBW of 45 [-] at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 1000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 1000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Shear modulus

G

25 - 26.5 GPa at 20 °C

Show 1000 Series materials with Shear modulus of 25 - 26.5 GPa at 20 °C

Tensile strength

Rm

150 - 160 MPa at 20 °C

Show 1000 Series materials with Tensile strength of 150 - 160 MPa at 20 °C

Tensile strength, transverse

Rm,trans

150 - 155 MPa at 20 °C

Show 1000 Series materials with Tensile strength, transverse of 150 - 155 MPa at 20 °C

Yield strength

YS

130 MPa at 20 °C

Show 1000 Series materials with Yield strength of 130 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

130 - 150 MPa at 20 °C

Show 1000 Series materials with Yield strength Rp0.2 of 130 - 150 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

130 - 140 MPa at 20 °C

Show 1000 Series materials with Yield strength Rp0.2, transverse of 130 - 140 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.17E-5 1/K at -50 °C

20-100°C

Unlock all property charts

Melting point

Tm

646 - 657 °C

Specific heat capacity

cp

899 - 900 J/(kg·K) at 20 °C

Thermal conductivity

λ

138 - 229 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

3.40E+7 - 3.60E+7 S/m at 20 °C

Electrical resistivity

ρel

2.78E-8 - 4.9E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Al

99.5 %

Fe

0.4 %

Si

0.1 - 0.25 %

B

0.05 %

Cu

0.05 %

More

Technological properties

Anodizing

Excellent

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Lithography; Cable Wrapping: Electric cable wrapping; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, rotor hub, stairs; Cosmetics: Cosmetics pieces; Automotive Trim: Interior Trim, Marque Badges; Components: Heat shields, General Transportation

Brazing

Excellent

Corrosion properties

Excellent

Welding

Excellent

Workability

Excellent

This material data has been provided by Aludium,WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.