EN 573-1 Grade AW-1070A H24

Want to keep this datasheet? Save it now in your required format

Description

Excellent surface finishing properties (bright, anodizing ...) and corrosion resistance.

Related Standards

Equivalent Materials

Ashby charts

See where EN 573-1 Grade AW-1070A H24 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.69 - 2.7 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.2 - 3 mm

Mechanical

Bending angle 180°

θ180

0.5 - 1 °/t at 20 °C

Show 1000 Series materials with Bending angle 180° of 0.5 - 1 °/t at 20 °C

Bending angle 90°

θ90

0 - 2.5 °/t at 20 °C

Show 1000 Series materials with Bending angle 90° of 0 - 2.5 °/t at 20 °C

according to EN 485-2

Elastic modulus

E

70 GPa at -270 °C

Show 1000 Series materials with Elastic modulus of 70 GPa at -270 °C

Hide chart

Elongation A50

A50

3 - 11 % at 20 °C

Show 1000 Series materials with Elongation A50 of 3 - 11 % at 20 °C

according to EN 485-2

Elongation A50, transverse

A50,trans

5 - 11 % at 20 °C

Show 1000 Series materials with Elongation A50, transverse of 5 - 11 % at 20 °C

Hardness, Brinell

HB

31 [-] at 20 °C

Show 1000 Series materials with Hardness, Brinell of 31 [-] at 20 °C

Hardness, HBW

HBW

31 - 35 [-] at 20 °C

Show 1000 Series materials with Hardness, HBW of 31 - 35 [-] at 20 °C

according to EN 485-2

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 1000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 1000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 1000 Series Aluminium

Shear modulus

G

25 - 26.5 GPa at 20 °C

Show 1000 Series materials with Shear modulus of 25 - 26.5 GPa at 20 °C

Tensile strength

Rm

100 - 150 MPa at 20 °C

Show 1000 Series materials with Tensile strength of 100 - 150 MPa at 20 °C

according to EN 485-2

Tensile strength, transverse

Rm,trans

100 - 140 MPa at 20 °C

Show 1000 Series materials with Tensile strength, transverse of 100 - 140 MPa at 20 °C

Yield strength

YS

60 - 80 MPa at 20 °C

Show 1000 Series materials with Yield strength of 60 - 80 MPa at 20 °C

according to EN 485-2

Yield strength Rp0.2

Rp0.2

60 MPa at 20 °C

Show 1000 Series materials with Yield strength Rp0.2 of 60 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

60 MPa at 20 °C

Show 1000 Series materials with Yield strength Rp0.2, transverse of 60 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.35E-5 1/K at 20 °C

20-100°C

Unlock all property charts

Melting point

Tm

659 °C

Specific heat capacity

cp

921 J/(kg·K) at 20 °C

Thermal conductivity

λ

138 - 225 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

3.45E+7 - 3.68E+7 S/m at 20 °C

Electrical resistivity

ρel

2.86E-8 - 4.9E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Al

99.7 %

Fe

0.25 %

Si

0.2 %

Zn

0.07 %

Cu

0.03 %

More

Technological properties

Anodizing

Excellent

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetic pieces; Automotive trim: Interior trim, Windows frame, Marque badges

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Corrosion properties

Excellent

Welding

Excellent

Workability

Excellent

This material data has been provided by Aludium,WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.