See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated Standards

Density

2.705 g/cm³

Show Material materials with Density of 2.705 g/cm³

H16

AA Standards

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H16

AA Standards

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 1000 Series Aluminium

Shear modulus

25.9 GPa

Show Material materials with Shear modulus of 25.9 GPa

Typical for Wrought 1000 Series Aluminium

Tensile strength

125.0 MPa

Show Material materials with Tensile strength of 125.0 MPa

H16

AA Standards

Thermal

PropertyTemperatureValueConditionRelated StandardsComment

Coefficient of thermal expansion

20 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

H16

AA Standards

100 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

H16

AA Standards

Melting point

645.0 - 655.0 °C

Show Material materials with Melting point of 645.0 - 655.0 °C

H16

AA Standards

Specific heat capacity

900.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 - 963.0 J/(kg·K)

Typical for Wrought 1000 Series Aluminium

Thermal conductivity

234 W/(m·K)

Show Material materials with Thermal conductivity of 234 W/(m·K)

H16

AA Standards

Electrical

PropertyValueConditionRelated Standards

Electrical conductivity

36000000.0 S/m

Show Material materials with Electrical conductivity of 36000000.0 S/m

H16

AA Standards

Electrical resistivity

2.78e-08 Ω·m

Show Material materials with Electrical resistivity of 2.78e-08 Ω·m

H16

AA Standards

Chemical properties

PropertyValueConditionRelated Standards

Aluminium

99.5 %

Show Material materials with Aluminium of 99.5 %

H16

AA Standards

Boron

0.05 %

Show Material materials with Boron of 0.05 %

H16

AA Standards

Chromium

0.01 %

Show Material materials with Chromium of 0.01 %

H16

AA Standards

Copper

0.05 %

Show Material materials with Copper of 0.05 %

H16

AA Standards

Gallium

0.03 %

Show Material materials with Gallium of 0.03 %

H16

AA Standards

Iron

0.40 %

Show Material materials with Iron of 0.40 %

H16

AA Standards

Manganese

0.01 %

Show Material materials with Manganese of 0.01 %

H16

AA Standards

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

H16

AA Standards

Zinc

0.05 %

Show Material materials with Zinc of 0.05 %

H16

AA Standards

Technological properties

Property
Brazing

general: possible with commercial processes and methods

Corrosion properties

Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere

General machinability

General: not suitable (O, H12, H111), poor (H14, H24, H16, H26, H18)

Workability

general (condition): good (O, H12, H111, H14, H24), acceptable (H16, H26, H18)