EN AW-1100 is a soft, non-heat-treatable and low strength alloy that offers strong corrosion resistance. Composed of 99% aluminum and 0.12% copper, EN AW-1100 is purest grade of aluminum alloy available commercially.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

H18

EN 573-3, EN 683

Strip, Sheet

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H18

EN 573-3, EN 683

Strip, Sheet

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 1000 Series Aluminium

Shear modulus

25.9 GPa

Show Material materials with Shear modulus of 25.9 GPa

Typical for Wrought 1000 Series Aluminium

Tensile strength

145.0 MPa

Show Material materials with Tensile strength of 145.0 MPa

H18

EN 573-3, EN 683

Strip, Sheet

20.0 °C

140.0 MPa

Show Material materials with Tensile strength of 140.0 MPa

H18

EN 573-3

Foil

20.0 °C

145.0 MPa

Show Material materials with Tensile strength of 145.0 MPa

H18

EN 573-3

Foil

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

H18

EN 573-3, EN 683

Strip, Sheet

100 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

H18

EN 573-3, EN 683

Strip, Sheet

Melting point

640.0 - 655.0 °C

Show Material materials with Melting point of 640.0 - 655.0 °C

H18

EN 573-3, EN 683

Strip, Sheet

Specific heat capacity

900.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 - 963.0 J/(kg·K)

Typical for Wrought 1000 Series Aluminium

Thermal conductivity

218.0 W/(m·K)

Show Material materials with Thermal conductivity of 218.0 W/(m·K)

H18

EN 573-3, EN 683

Strip, Sheet

218.0 - 222.0 W/(m·K)

Show Material materials with Thermal conductivity of 218.0 - 222.0 W/(m·K)

H18

EN 573-3, EN 683

Strip, Sheet

Electrical

PropertyValueConditionRelated StandardsShape

Electrical conductivity

33000000.0 S/m

Show Material materials with Electrical conductivity of 33000000.0 S/m

H18

EN 573-3, EN 683

Strip, Sheet

33000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 33000000.0 - 34000000.0 S/m

H18

EN 573-3, EN 683

Strip, Sheet

Electrical resistivity

2.94e-08 - 3.03e-08 Ω·m

Show Material materials with Electrical resistivity of 2.94e-08 - 3.03e-08 Ω·m

H18

EN 573-3, EN 683

Strip, Sheet

3.03e-08 Ω·m

Show Material materials with Electrical resistivity of 3.03e-08 Ω·m

H18

EN 573-3, EN 683

Strip, Sheet

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

99.0 %

Show Material materials with Aluminium of 99.0 %

H18

EN 573-3, EN 683

Foil, Strip, Sheet

Copper

0.05 - 0.2 %

Show Material materials with Copper of 0.05 - 0.2 %

H18

EN 573-3, EN 683

Foil, Strip, Sheet

Manganese

0.05 %

Show Material materials with Manganese of 0.05 %

H18

EN 573-3, EN 683

Foil, Strip, Sheet

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

H18

EN 573-3, EN 683

Foil, Strip, Sheet

Technological properties

Property
Brazing

Excellent

Workability

Excellent workability.