AA Standards Grade 7075 T73

Want to keep this datasheet? Save it now in your required format

Description

AA 7075 is a high-strength alloy that offers good stress-corrosion cracking resistance. Known as a mainstay in the aerospace industry since it was introduced, Aluminum 7075 brings moderate toughness as well as an excellent strength-to-weight ratio. It is also important to note that at sub-zero temperatures Aluminum 7075 increases in strength.

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.7 - 2.85 g/cm³

Show Material materials with Density of 2.7 - 2.85 g/cm³

Typical for Wrought 7000 Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

69.0 - 72.0 GPa

Show Material materials with Elastic modulus of 69.0 - 72.0 GPa

Typical for Wrought 7000 Series Aluminium

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 7000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 7000 Series Aluminium

Shear modulus

26.4 - 27.1 GPa

Show Material materials with Shear modulus of 26.4 - 27.1 GPa

Typical for Wrought 7000 Series Aluminium

Tensile strength

395.0 MPa

Show Material materials with Tensile strength of 395.0 MPa

T73

AA Standards, ASTM B247

400.0 MPa

Show Material materials with Tensile strength of 400.0 MPa

T73

AA Standards, ASTM B247

405.0 MPa

Show Material materials with Tensile strength of 405.0 MPa

T73

AA Standards, ASTM B247

415.0 MPa

Show Material materials with Tensile strength of 415.0 MPa

T73

AA Standards, ASTM B247

420.0 MPa

Show Material materials with Tensile strength of 420.0 MPa

T73

AA Standards, ASTM B247

425.0 MPa

Show Material materials with Tensile strength of 425.0 MPa

T73

AA Standards, ASTM B247

435.0 MPa

Show Material materials with Tensile strength of 435.0 MPa

T73

AA Standards, ASTM B247

440.0 MPa

Show Material materials with Tensile strength of 440.0 MPa

T73

AA Standards, ASTM B211, ASTM B247

450.0 MPa

Show Material materials with Tensile strength of 450.0 MPa

T73

AA Standards, ASTM B221

455.0 MPa

Show Material materials with Tensile strength of 455.0 MPa

T73

AA Standards, ASTM B210, ASTM B211, ASTM B247

460.0 MPa

Show Material materials with Tensile strength of 460.0 MPa

T73

AA Standards, ASTM B209

470.0 MPa

Show Material materials with Tensile strength of 470.0 MPa

T73

AA Standards, ASTM B211, ASTM B221, ASTM B241, ASTM B316

475.0 MPa

Show Material materials with Tensile strength of 475.0 MPa

T73

AA Standards, ASTM B221, ASTM B241

485.0 MPa

Show Material materials with Tensile strength of 485.0 MPa

T73

AA Standards, ASTM B221, ASTM B241

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.1e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1e-05 - 2.4e-05 1/K

Typical for Wrought 7000 Series Aluminium

Melting point

465.0 - 655.0 °C

Show Material materials with Melting point of 465.0 - 655.0 °C

Typical for Wrought 7000 Series Aluminium

Specific heat capacity

795.0 - 1050.0 J/(kg·K)

Show Material materials with Specific heat capacity of 795.0 - 1050.0 J/(kg·K)

Typical for Wrought 7000 Series Aluminium

Thermal conductivity

121.0 - 170.0 W/(m·K)

Show Material materials with Thermal conductivity of 121.0 - 170.0 W/(m·K)

Typical for Wrought 7000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 34000000.0 S/m

Typical for Wrought 7000 Series Aluminium

Electrical resistivity

2.9e-08 - 5.6e-08 Ω·m

Show Material materials with Electrical resistivity of 2.9e-08 - 5.6e-08 Ω·m

Typical for Wrought 7000 Series Aluminium

Chemical properties

PropertyValueConditionRelated Standards

Chromium

0.18 - 0.28 %

Show Material materials with Chromium of 0.18 - 0.28 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Copper

1.2 - 2.0 %

Show Material materials with Copper of 1.2 - 2.0 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Iron

0.50 %

Show Material materials with Iron of 0.50 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Magnesium

2.1 - 2.9 %

Show Material materials with Magnesium of 2.1 - 2.9 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Manganese

0.3 %

Show Material materials with Manganese of 0.3 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Titanium

0.2 %

Show Material materials with Titanium of 0.2 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Zinc

5.1 - 6.1 %

Show Material materials with Zinc of 5.1 - 6.1 %

T73

AA Standards, ASTM B209, ASTM B210, ASTM B211, ASTM B221, ASTM B241, ASTM B247, ASTM B316

Technological properties

Property
Brazing

general: no brazing is known or developed

Corrosion properties

Stress corrosion cracking: Operational damage in areas with tensile stresses transverse to the grain structure, limited damage to laboratory samples, general: good, without protection in industrial or seawater atmosphere

General machinability

General: poor (O), good to acceptable

Workability

general (condition): not suitable