EN 573-3 Grade AW-2011 H13

Want to keep this datasheet? Save it now in your required format

Description

Aluminum EN AW-2011 is a popular age-hardenable alloy known for its free-machining characteristics and mechanical properties. It can be machined to very close tolerances while still maintaining a smooth and bright finish. Unlike other aluminum alloys, EN AW-2011 does not offer good corrosion resistance or weldability.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20.0 °C

2.82 g/cm³

Show Material materials with Density of 2.82 g/cm³

H13

EN 573-3

Wire

2.82 g/cm³

Show Material materials with Density of 2.82 g/cm³

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

2.83 g/cm³

Show Material materials with Density of 2.83 g/cm³

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

72.5 GPa

Show Material materials with Elastic modulus of 72.5 GPa

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 2000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 2000 Series Aluminium

Shear modulus

27.3 GPa

Show Material materials with Shear modulus of 27.3 GPa

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Tensile strength

155.0 - 225.0 MPa

Show Material materials with Tensile strength of 155.0 - 225.0 MPa

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

300 °C, 20 °C

2.4999999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4999999999999998e-05 1/K

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

200 °C, 20 °C, 200.0 °C

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar, Wire

100 °C, 20 °C

2.3399999999999996e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

20 °C, -50 °C, -50.0 °C

2.14e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.14e-05 1/K

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar, Wire

100 °C, 20 °C

2.2899999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2899999999999998e-05 1/K

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

100.0 °C

2.29e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.29e-05 1/K

H13

EN 573-3

Wire

100.0 °C

2.29e-05 - 2.31e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.29e-05 - 2.31e-05 1/K

H13

EN 573-3

Wire

100.0 °C

2.31e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.31e-05 1/K

H13

EN 573-3

Wire

300.0 °C

2.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5e-05 1/K

H13

EN 573-3

Wire

Melting point

585.0 - 650.0 °C

Show Material materials with Melting point of 585.0 - 650.0 °C

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

540.0 - 645.0 °C

Show Material materials with Melting point of 540.0 - 645.0 °C

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Specific heat capacity

20.0 °C

864.0 J/(kg·K)

Show Material materials with Specific heat capacity of 864.0 J/(kg·K)

H13

EN 573-3

Wire

864.0 J/(kg·K)

Show Material materials with Specific heat capacity of 864.0 J/(kg·K)

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Thermal conductivity

20.0 °C

151.0 - 172.0 W/(m·K)

Show Material materials with Thermal conductivity of 151.0 - 172.0 W/(m·K)

H13

EN 573-3, EN 1301

Wire, Strip, Sheet, Plate, Tube, Bar

170.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 170.0 - 220.0 W/(m·K)

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

23000000.0 - 26000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 26000000.0 S/m

H13

EN 573-3, EN 1301

Wire, Strip, Sheet, Plate, Tube, Bar

24000000.0 - 32000000.0 S/m

Show Material materials with Electrical conductivity of 24000000.0 - 32000000.0 S/m

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Electrical resistivity

3.13e-08 - 4.17e-08 Ω·m

Show Material materials with Electrical resistivity of 3.13e-08 - 4.17e-08 Ω·m

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

3.85e-08 - 4.35e-08 Ω·m

Show Material materials with Electrical resistivity of 3.85e-08 - 4.35e-08 Ω·m

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Chemical properties

PropertyValueConditionRelated StandardsShape

Bismuth

0.2 - 0.6 %

Show Material materials with Bismuth of 0.2 - 0.6 %

H13

EN 573-3, EN 1301

Wire, Strip, Sheet, Plate, Tube, Bar

Copper

5.0 - 6.0 %

Show Material materials with Copper of 5.0 - 6.0 %

H13

EN 573-3, EN 1301

Wire, Strip, Sheet, Plate, Tube, Bar

Iron

0.7 %

Show Material materials with Iron of 0.7 %

H13

EN 573-3

Wire

0.70 %

Show Material materials with Iron of 0.70 %

H13

EN 573-3, EN 1301

Strip, Sheet, Plate, Tube, Bar

Lead

0.2 - 0.6 %

Show Material materials with Lead of 0.2 - 0.6 %

H13

EN 573-3, EN 1301

Wire, Strip, Sheet, Plate, Tube, Bar

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

H13

EN 573-3, EN 1301

Wire, Strip, Sheet, Plate, Tube, Bar

Zinc

0.3 %

Show Material materials with Zinc of 0.3 %

H13

EN 573-3, EN 1301

Wire, Strip, Sheet, Plate, Tube, Bar

Technological properties

Property
Anodizing

decorative: not suitable, Protective: poor

Brazing

hard brazing (with flux/ without flux): not suitable /, friction soldering: sufficient

Corrosion properties

Seawater: poor, weathering: sufficient

Workability

Deep drawing / upsetting (Condition) - / acceptable