EN 573-3 Grade AW-2618A T6511

Want to keep this datasheet? Save it now in your required format

Description

Age-hardenable AlCu alloy. The alloy is not food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.77 g/cm³

Show Material materials with Density of 2.77 g/cm³

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 - 73.0 GPa

Show Material materials with Elastic modulus of 70.0 - 73.0 GPa

Typical for Wrought 2000 Series Aluminium

Elongation

4.0 %

Show Material materials with Elongation of 4.0 %

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

A50

5.0 %

Show Material materials with Elongation of 5.0 %

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

A50

6.0 %

Show Material materials with Elongation of 6.0 %

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

7.0 %

Show Material materials with Elongation of 7.0 %

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

20.0 °C

4.0 %

Show Material materials with Elongation of 4.0 %

T6511

EN 573-3

Profile, Rod, Tube

A50

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

T6511

EN 573-3

Profile, Rod, Tube

A50

20.0 °C

6.0 %

Show Material materials with Elongation of 6.0 %

T6511

EN 573-3

Profile, Rod, Tube

20.0 °C

7.0 %

Show Material materials with Elongation of 7.0 %

T6511

EN 573-3

Profile, Rod, Tube

Hardness, Brinell

140.0 [-]

Show Material materials with Hardness, Brinell of 140.0 [-]

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

145.0 [-]

Show Material materials with Hardness, Brinell of 145.0 [-]

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

20.0 °C

140.0 [-]

Show Material materials with Hardness, Brinell of 140.0 [-]

T6511

EN 573-3

Profile, Rod, Tube

20.0 °C

140.0 - 145.0 [-]

Show Material materials with Hardness, Brinell of 140.0 - 145.0 [-]

T6511

EN 573-3

Profile, Rod, Tube

20.0 °C

145.0 [-]

Show Material materials with Hardness, Brinell of 145.0 [-]

T6511

EN 573-3

Profile, Rod, Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 2000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 2000 Series Aluminium

Shear modulus

26.0 - 27.5 GPa

Show Material materials with Shear modulus of 26.0 - 27.5 GPa

Typical for Wrought 2000 Series Aluminium

Tensile strength

410.0 MPa

Show Material materials with Tensile strength of 410.0 MPa

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

420.0 MPa

Show Material materials with Tensile strength of 420.0 MPa

T6511

EN 573-3, EN 755

Strip, Sheet, Plate

20.0 °C

410.0 MPa

Show Material materials with Tensile strength of 410.0 MPa

T6511

EN 573-3

Profile, Rod, Tube

20.0 °C

420.0 MPa

Show Material materials with Tensile strength of 420.0 MPa

T6511

EN 573-3

Profile, Rod, Tube

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.6e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.4e-05 1/K

Typical for Wrought 2000 Series Aluminium

Melting point

500.0 - 650.0 °C

Show Material materials with Melting point of 500.0 - 650.0 °C

Typical for Wrought 2000 Series Aluminium

Specific heat capacity

816.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 816.0 - 963.0 J/(kg·K)

Typical for Wrought 2000 Series Aluminium

Thermal conductivity

112.0 - 251.0 W/(m·K)

Show Material materials with Thermal conductivity of 112.0 - 251.0 W/(m·K)

Typical for Wrought 2000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 30000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 30000000.0 S/m

Typical for Wrought 2000 Series Aluminium

Electrical resistivity

3.4e-08 - 6e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 6e-08 Ω·m

Typical for Wrought 2000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

1.8 - 2.7 %

Show Material materials with Copper of 1.8 - 2.7 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Iron

0.9 - 1.4 %

Show Material materials with Iron of 0.9 - 1.4 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Magnesium

1.2 - 1.8 %

Show Material materials with Magnesium of 1.2 - 1.8 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Manganese

0.25 %

Show Material materials with Manganese of 0.25 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Nickel

0.8 - 1.4 %

Show Material materials with Nickel of 0.8 - 1.4 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Silicon

0.15 - 0.25 %

Show Material materials with Silicon of 0.15 - 0.25 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Titanium

0.2 %

Show Material materials with Titanium of 0.2 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Zinc

0.15 %

Show Material materials with Zinc of 0.15 %

T6511

EN 573-3, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate

Technological properties

Property
Workability

Moderate Workability