EN 573-3 Grade AW-8006 H24

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlFeMn alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,Aludium,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.74 g/cm³

Show Material materials with Density of 2.74 g/cm³

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

2.74 g/cm³

Show Material materials with Density of 2.74 g/cm³

H24

EN 573-3, EN 546, EN 683

Strip, Sheet

Dimension

PropertyValueConditionRelated StandardsThicknessShape

Thickness

0.06 mm

Show Material materials with Thickness of 0.06 mm

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

0.06 mm

Coil, Foil

0.2 mm

Show Material materials with Thickness of 0.2 mm

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

0.2 mm

Coil, Foil

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 8000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 8000 Series Aluminium

Shear modulus

25.0 GPa

Show Material materials with Shear modulus of 25.0 GPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Tensile strength

20.0 °C

110.0 - 170.0 MPa

Show Material materials with Tensile strength of 110.0 - 170.0 MPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2, EN 573-3, EN 546, EN 683

Coil, Foil, Strip, Sheet, Foil

20.0 °C

120.0 - 160.0 MPa

Show Material materials with Tensile strength of 120.0 - 160.0 MPa

H24

EN 573-3

Foil

Yield strength

90.0 MPa

Show Material materials with Yield strength of 90.0 MPa

H24

EN 573-3, EN 683

Strip, Sheet

RP02

90 MPa

Show Material materials with Yield strength of 90 MPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

20.0 °C

90.0 MPa

Show Material materials with Yield strength of 90.0 MPa

H24

EN 573-3

Foil

RP02

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

100 °C

0.000024 1/K

Show Material materials with Coefficient of thermal expansion of 0.000024 1/K

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

20-100°C

Melting point

645.0 - 655.0 °C

Show Material materials with Melting point of 645.0 - 655.0 °C

Typical for Wrought 8000 Series Aluminium

Specific heat capacity

920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 920.0 J/(kg·K)

Typical for Wrought 8000 Series Aluminium

Thermal conductivity

190.0 - 210.0 W/(m·K)

Show Material materials with Thermal conductivity of 190.0 - 210.0 W/(m·K)

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Electrical

PropertyValueConditionRelated StandardsShapeComment

Electrical conductivity

28000000.0 - 35000000.0 S/m

Show Material materials with Electrical conductivity of 28000000.0 - 35000000.0 S/m

Typical for Wrought 8000 Series Aluminium

Electrical resistivity

3.1e-08 Ω·m

Show Material materials with Electrical resistivity of 3.1e-08 Ω·m

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.3 %

Show Material materials with Copper of 0.3 %

H24

EN 573-3, EN 546, EN 683

Foil, Strip, Sheet

0.3 %

Show Material materials with Copper of 0.3 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Iron

1.2 - 2.0 %

Show Material materials with Iron of 1.2 - 2.0 %

H24

EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2, EN 546, EN 683

Foil, Coil, Foil, Strip, Sheet

Magnesium

0.1 %

Show Material materials with Magnesium of 0.1 %

H24

EN 573-3, EN 546, EN 683

Foil, Strip, Sheet

0.1 %

Show Material materials with Magnesium of 0.1 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Manganese

0.3 - 1.0 %

Show Material materials with Manganese of 0.3 - 1.0 %

H24

EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2, EN 546, EN 683

Foil, Coil, Foil, Strip, Sheet

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

H24

EN 573-3, EN 546, EN 683

Foil, Strip, Sheet

0.4 %

Show Material materials with Silicon of 0.4 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

H24

EN 573-3, EN 546, EN 683

Foil, Strip, Sheet

0.1 %

Show Material materials with Zinc of 0.1 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 683-2

Coil, Foil

Technological properties

Property
Anodizing

Limited

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels; Electronic devices: Housing of devices; Heat exchangers: Fins, Heat exchangers, General applications; Tubes: Industrial tubes, Flexible tubes, Pipes; Insulation; Semi-rigid and corrugated: Pet food, Smooth wall; Components: Automotive fins, Heat exchangers

Corrosion properties

Limited

Welding

Good

Workability

Very Good