EN 573-3 Grade AW-8011A F

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlFeSi alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil

20.0 °C

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

F

EN 573-3

Flat

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 8000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 8000 Series Aluminium

Tensile strength

85.0 MPa

Show Material materials with Tensile strength of 85.0 MPa

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil

20.0 °C

85.0 MPa

Show Material materials with Tensile strength of 85.0 MPa

F

EN 573-3

Flat

Transverse

20.0 °C

85.0 MPa

Show Material materials with Tensile strength of 85.0 MPa

F

EN 573-3

Flat

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil

100 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil

Melting point

640.0 - 655.0 °C

Show Material materials with Melting point of 640.0 - 655.0 °C

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil

Specific heat capacity

920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 920.0 J/(kg·K)

Typical for Wrought 8000 Series Aluminium

Thermal conductivity

20.0 °C

210.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 210.0 - 220.0 W/(m·K)

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

34000000.0 - 35000000.0 S/m

Show Material materials with Electrical conductivity of 34000000.0 - 35000000.0 S/m

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Electrical resistivity

2.86e-08 - 2.94e-08 Ω·m

Show Material materials with Electrical resistivity of 2.86e-08 - 2.94e-08 Ω·m

F

EN 573-3, EN 485

Strip, Sheet, Plate, Foil

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Copper

0.1 %

Show Material materials with Copper of 0.1 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Iron

0.5 - 1.0 %

Show Material materials with Iron of 0.5 - 1.0 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Magnesium

0.1 %

Show Material materials with Magnesium of 0.1 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Silicon

0.4 - 0.8 %

Show Material materials with Silicon of 0.4 - 0.8 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

F

EN 573-3, EN 485

Flat, Strip, Sheet, Plate, Foil

Technological properties

Property
Anodizing

decorative: acceptable, Protective: very good

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Corrosion properties

Seawater: sufficient, weathering: acceptable

Workability

Bending / Spinning (cold): good / good, Impact extrusion (cold): good, Deep drawing / upsetting (Condition) good (H14) / good (H14)