EN 573-3 Grade AW-3105A H24

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlMn alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,Aludium,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

H24

EN 573-3, EN 541

Strip, Sheet, Plate

Dimension

PropertyValueConditionRelated StandardsThicknessShape

Thickness

0.18 mm

Show Material materials with Thickness of 0.18 mm

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

0.18 mm

Coil, Sheet

1.0 mm

Show Material materials with Thickness of 1.0 mm

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

1.0 mm

Coil, Sheet

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending angle 180°

2.5 °/t

Show Material materials with Bending angle 180° of 2.5 °/t

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Hardness, HBW

48 [-]

Show Material materials with Hardness, HBW of 48 [-]

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

26.0 GPa

Show Material materials with Shear modulus of 26.0 GPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Tensile strength

150.0 - 240.0 MPa

Show Material materials with Tensile strength of 150.0 - 240.0 MPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

20.0 °C

150.0 - 190.0 MPa

Show Material materials with Tensile strength of 150.0 - 190.0 MPa

H24

EN 573-3, EN 541

Sheet, Strip, Plate

Yield strength

120.0 - 220.0 MPa

Show Material materials with Yield strength of 120.0 - 220.0 MPa

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

20.0 °C

120.0 - 160.0 MPa

Show Material materials with Yield strength of 120.0 - 160.0 MPa

H24

EN 573-3, EN 541

Sheet, Strip, Plate

RP02

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

100 °C

0.000024 1/K

Show Material materials with Coefficient of thermal expansion of 0.000024 1/K

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

20-100°C

Melting point

629.0 - 654.0 °C

Show Material materials with Melting point of 629.0 - 654.0 °C

Typical for Wrought 3000 Series Aluminium

Specific heat capacity

893.0 - 920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 - 920.0 J/(kg·K)

Typical for Wrought 3000 Series Aluminium

Thermal conductivity

172 W/(m·K)

Show Material materials with Thermal conductivity of 172 W/(m·K)

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Electrical

PropertyValueConditionRelated StandardsShapeComment

Electrical conductivity

23000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m

Typical for Wrought 3000 Series Aluminium

Electrical resistivity

3.7999999999999996e-08 Ω·m

Show Material materials with Electrical resistivity of 3.7999999999999996e-08 Ω·m

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.2 %

Show Material materials with Chromium of 0.2 %

H24

EN 573-3, EN 541

Sheet, Strip, Plate

0.2 %

Show Material materials with Chromium of 0.2 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Copper

0.3 %

Show Material materials with Copper of 0.3 %

H24

EN 573-3, EN 541

Sheet, Strip, Plate

0.3 %

Show Material materials with Copper of 0.3 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Iron

0.7 %

Show Material materials with Iron of 0.7 %

H24

EN 573-3

Sheet

0.7 %

Show Material materials with Iron of 0.7 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

0.70 %

Show Material materials with Iron of 0.70 %

H24

EN 573-3, EN 541

Strip, Sheet, Plate

Magnesium

0.2 - 0.8 %

Show Material materials with Magnesium of 0.2 - 0.8 %

H24

EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541

Sheet, Coil, Sheet, Strip, Plate

Manganese

0.3 - 0.8 %

Show Material materials with Manganese of 0.3 - 0.8 %

H24

EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541

Sheet, Coil, Sheet, Strip, Plate

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

H24

EN 573-3, EN 541

Sheet, Strip, Plate

0.6 %

Show Material materials with Silicon of 0.6 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

H24

EN 573-3, EN 541

Sheet, Strip, Plate

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

H24

EN 573-3, EN 541

Sheet, Strip, Plate

0.25 %

Show Material materials with Zinc of 0.25 %

H24

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Technological properties

Property
Anodizing

Good

Application areas

Closures: Short cups; Food can: Body, Lids; Semi-rigid and corrugated: Pet food

Brazing

Good

Corrosion properties

Very Good

Welding

Very Good

Workability

Very Good