Properties

General

Density

ρ

2.71 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Mechanical

Elastic modulus

E

69 - 71 GPa at 20 °C

Show 4000 Series materials with Elastic modulus of 69 - 71 GPa at 20 °C

Typical for Wrought 4000 Series Aluminium

Elongation A50

A50

20 % at 20 °C

Show 4000 Series materials with Elongation A50 of 20 % at 20 °C

Hardness, Brinell

HB

35 [-] at 20 °C

Show 4000 Series materials with Hardness, Brinell of 35 [-] at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 4000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 4000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 4000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 4000 Series Aluminium

Shear modulus

G

26 GPa at 20 °C

Show 4000 Series materials with Shear modulus of 26 GPa at 20 °C

Typical for Wrought 4000 Series Aluminium

Tensile strength

Rm

150 MPa at 20 °C

Show 4000 Series materials with Tensile strength of 150 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

45 - 90 MPa at 20 °C

Show 4000 Series materials with Yield strength Rp0.2 of 45 - 90 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 - 2.2E-5 1/K at 20 °C

Typical for Wrought 4000 Series Aluminium

Specific heat capacity

cp

864 J/(kg·K) at 20 °C

Typical for Wrought 4000 Series Aluminium

Thermal conductivity

λ

138 - 155 W/(m·K) at 20 °C

Typical for Wrought 4000 Series Aluminium

Electrical

Electrical conductivity

σel

2.30E+7 - 3.00E+7 S/m at 20 °C

Typical for Wrought 4000 Series Aluminium

Electrical resistivity

ρel

3.8E-8 - 5E-8 Ω·m at 20 °C

Typical for Wrought 4000 Series Aluminium

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Si

1.4 - 2.2 %

Fe

0.7 %

Mn

0.6 - 1.2 %

Cu

0.2 %

More

Technological properties

Workability

Moderate Workability

This material data has been provided by WIAM,AluKey.