General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | |
20.0 °C | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | H19 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Flat, Coil, Sheet, Strip |
Dimension
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Thickness | 0.1 mm Show Material materials with Thickness of 0.1 mm | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | 0.1 mm | Coil, Sheet, Strip |
4.0 mm Show Material materials with Thickness of 4.0 mm | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | 4.0 mm | Coil, Sheet, Strip |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending angle 180° | 0 °/t Show Material materials with Bending angle 180° of 0 °/t | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | ||
Bending angle 90° | 0 °/t Show Material materials with Bending angle 90° of 0 °/t | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | ||
Elastic modulus | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | ||
69.5 GPa Show Material materials with Elastic modulus of 69.5 GPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | |||
70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |||
20.0 °C | 69.5 GPa Show Material materials with Elastic modulus of 69.5 GPa | H19 | EN 573-3 | Flat | ||
Hardness, Brinell | 64.0 [-] Show Material materials with Hardness, Brinell of 64.0 [-] | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | ||
20.0 °C | 64.0 [-] Show Material materials with Hardness, Brinell of 64.0 [-] | H19 | EN 573-3 | Flat | ||
Hardness, HBW | 64 [-] Show Material materials with Hardness, HBW of 64 [-] | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 20.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | H19 | EN 573-3 | Flat | |
Shear modulus | 26.1 GPa Show Material materials with Shear modulus of 26.1 GPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | ||
26.5 GPa Show Material materials with Shear modulus of 26.5 GPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |||
20.0 °C | 26.1 GPa Show Material materials with Shear modulus of 26.1 GPa | H19 | EN 573-3 | Flat | ||
Tensile strength | 205.0 MPa Show Material materials with Tensile strength of 205.0 MPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | ||
205 MPa Show Material materials with Tensile strength of 205 MPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |||
20.0 °C | 205.0 MPa Show Material materials with Tensile strength of 205.0 MPa | H19 | EN 573-3 | Flat | Transverse | |
20.0 °C | 205.0 MPa Show Material materials with Tensile strength of 205.0 MPa | H19 | EN 573-3 | Flat | ||
Yield strength | 185.0 MPa Show Material materials with Yield strength of 185.0 MPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | RP02 | |
185 MPa Show Material materials with Yield strength of 185 MPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |||
20.0 °C | 185.0 MPa Show Material materials with Yield strength of 185.0 MPa | H19 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 185.0 MPa Show Material materials with Yield strength of 185.0 MPa | H19 | EN 573-3 | Flat | RP02 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | |
100 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | ||
100 °C | 0.000024 1/K Show Material materials with Coefficient of thermal expansion of 0.000024 1/K | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | 20-100°C | |
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Melting point | 630.0 - 655.0 °C Show Material materials with Melting point of 630.0 - 655.0 °C | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | ||
Specific heat capacity | 20.0 °C | 897.0 J/(kg·K) Show Material materials with Specific heat capacity of 897.0 J/(kg·K) | H19 | EN 573-3 | Flat | |
Thermal conductivity | 200 W/(m·K) Show Material materials with Thermal conductivity of 200 W/(m·K) | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | ||
201 W/(m·K) Show Material materials with Thermal conductivity of 201 W/(m·K) | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | |||
20.0 °C | 201.0 W/(m·K) Show Material materials with Thermal conductivity of 201.0 W/(m·K) | H19 | EN 573-3 | Flat |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Electrical conductivity | 30000000.0 S/m Show Material materials with Electrical conductivity of 30000000.0 S/m | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | |
Electrical resistivity | 3.33e-08 Ω·m Show Material materials with Electrical resistivity of 3.33e-08 Ω·m | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | |
20.0 °C | 3.3e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 Ω·m | H19 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Flat, Coil, Sheet, Strip |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate, Tube, Welded Tube, Bar |
0.1 % Show Material materials with Chromium of 0.1 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |
Copper | 0.2 % Show Material materials with Copper of 0.2 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate, Tube, Welded Tube, Bar |
0.2 % Show Material materials with Copper of 0.2 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |
Iron | 0.7 % Show Material materials with Iron of 0.7 % | H19 | EN 573-3 | Flat |
0.70 % Show Material materials with Iron of 0.70 % | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Welded Tube, Bar | |
0.7 % Show Material materials with Iron of 0.7 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |
Magnesium | 0.5 - 1.1 % Show Material materials with Magnesium of 0.5 - 1.1 % | H19 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Flat, Strip, Sheet, Plate, Tube, Welded Tube, Bar, Coil, Sheet, Strip |
Manganese | 0.2 % Show Material materials with Manganese of 0.2 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate, Tube, Welded Tube, Bar |
0.2 % Show Material materials with Manganese of 0.2 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |
Silicon | 0.3 % Show Material materials with Silicon of 0.3 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate, Tube, Welded Tube, Bar |
0.3 % Show Material materials with Silicon of 0.3 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip | |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate, Tube, Welded Tube, Bar |
0.25 % Show Material materials with Zinc of 0.25 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2 | Coil, Sheet, Strip |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: acceptable, Protective: very good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Anodizing quality; Heat exchangers: Fins, General applications; Cosmetics: Cosmetics pieces; Automotive trim: Interior trim; Components: Automotive fins, Heat exchangers | |
Brazing | hard brazing (with flux/ without flux): acceptable / sufficient, friction soldering: good, soft brazing with flux: sufficient | |
Corrosion properties | Seawater: good, weathering: very good | |
Welding | Very Good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) good (O) / good (O) |