EN 573-3 Grade AW-5010 H46

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlMg alloy. The alloy is not food safe.

Related Standards

Equivalent Materials

Ashby charts

See where EN 573-3 Grade AW-5010 H46 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.7 - 2.71 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Mechanical

Elastic modulus

E

69 - 70 GPa at 20 °C

Show 5000 Series materials with Elastic modulus of 69 - 70 GPa at 20 °C

Typical for Wrought 5000 Series Aluminium

Elongation A50

A50

2 - 3 % at 20 °C

Show 5000 Series materials with Elongation A50 of 2 - 3 % at 20 °C

Elongation A50, transverse

A50,trans

2 - 3 % at 20 °C

Show 5000 Series materials with Elongation A50, transverse of 2 - 3 % at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 5000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 5000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 5000 Series Aluminium

Shear modulus

G

27 GPa at 20 °C

Show 5000 Series materials with Shear modulus of 27 GPa at 20 °C

Tensile strength

Rm

150 - 190 MPa at 20 °C

Show 5000 Series materials with Tensile strength of 150 - 190 MPa at 20 °C

Tensile strength, transverse

Rm,trans

150 - 190 MPa at 20 °C

Show 5000 Series materials with Tensile strength, transverse of 150 - 190 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

120 MPa at 20 °C

Show 5000 Series materials with Yield strength Rp0.2 of 120 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

120 MPa at 20 °C

Show 5000 Series materials with Yield strength Rp0.2, transverse of 120 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.2E-5 - 2.5E-5 1/K at 20 °C

Typical for Wrought 5000 Series Aluminium

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

600 - 650 °C

Typical for Wrought 5000 Series Aluminium

Specific heat capacity

cp

879 - 963 J/(kg·K) at 20 °C

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

λ

215 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

3.50E+7 S/m at 20 °C

Electrical resistivity

ρel

3.3E-8 - 5E-8 Ω·m at 20 °C

Typical for Wrought 5000 Series Aluminium

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Fe

0.7 %

Si

0.4 %

Zn

0.3 %

Cu

0.25 %

More

Technological properties

Workability

Good workability.

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.