EN 573-3 Grade AW-5042 O

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlMg alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey,Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.67 g/cm³

Show Material materials with Density of 2.67 g/cm³

O

EN 573-3, EN 485

2.67 g/cm³

Show Material materials with Density of 2.67 g/cm³

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending angle 180°

2.0 °/t

Show Material materials with Bending angle 180° of 2.0 °/t

O

EN 573-3, EN 485

1.5 °/t

Show Material materials with Bending angle 180° of 1.5 °/t

O

EN 573-3, EN 485

Elastic modulus

71.0 GPa

Show Material materials with Elastic modulus of 71.0 GPa

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Elongation

20.0 °C

18.0 %

Show Material materials with Elongation of 18.0 %

O

EN 573-3

Flat

A50 Transverse

20.0 °C

18.0 %

Show Material materials with Elongation of 18.0 %

O

EN 573-3

Flat

Transverse

18.0 %

Show Material materials with Elongation of 18.0 %

O

EN 573-3, EN 485

18.0 %

Show Material materials with Elongation of 18.0 %

O

EN 573-3, EN 485

A50

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

27.6 GPa

Show Material materials with Shear modulus of 27.6 GPa

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Tensile strength

20.0 °C

240.0 - 350.0 MPa

Show Material materials with Tensile strength of 240.0 - 350.0 MPa

O

EN 573-3

Flat

Transverse

240.0 - 350.0 MPa

Show Material materials with Tensile strength of 240.0 - 350.0 MPa

O

EN 573-3, EN 485

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

100 °C

0.000024 1/K

Show Material materials with Coefficient of thermal expansion of 0.000024 1/K

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

20-100°C

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

560.0 - 655.0 °C

Show Material materials with Melting point of 560.0 - 655.0 °C

Typical for Wrought 5000 Series Aluminium

Specific heat capacity

879.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K)

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

125 W/(m·K)

Show Material materials with Thermal conductivity of 125 W/(m·K)

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Electrical

PropertyValueConditionRelated StandardsShapeComment

Electrical conductivity

18000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

5.7e-08 Ω·m

Show Material materials with Electrical resistivity of 5.7e-08 Ω·m

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

O

EN 573-3, EN 485

Flat

0.1 %

Show Material materials with Chromium of 0.1 %

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Copper

0.15 %

Show Material materials with Copper of 0.15 %

O

EN 573-3, EN 485

Flat

0.15 %

Show Material materials with Copper of 0.15 %

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Iron

0.35 %

Show Material materials with Iron of 0.35 %

O

EN 573-3

Flat

0.35 %

Show Material materials with Iron of 0.35 %

O

EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Magnesium

3.0 - 4.0 %

Show Material materials with Magnesium of 3.0 - 4.0 %

O

EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Flat, Coil, Sheet, Plate

Manganese

0.2 - 0.5 %

Show Material materials with Manganese of 0.2 - 0.5 %

O

EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Flat, Coil, Sheet, Plate

Other

0.05 - 0.15 %

Show Material materials with Other of 0.05 - 0.15 %

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Silicon

0.2 %

Show Material materials with Silicon of 0.2 %

O

EN 573-3, EN 485

Flat

0.2 %

Show Material materials with Silicon of 0.2 %

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

O

EN 573-3

Flat

0.1 %

Show Material materials with Titanium of 0.1 %

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

O

EN 573-3, EN 485

Flat

0.25 %

Show Material materials with Zinc of 0.25 %

O

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet, Plate

Technological properties

Property
Anodizing

Excellent (anodizing quality)

Application areas

Vessels: Pressure; Wind energy: Nacelle coverings, rotor hub, stairs; Food can: Body, Lids; Components: Access hatches, Spoilers, General transportation

Corrosion properties

Excellent

Welding

Good

Workability

Good (in O temper)