General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Density | 2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate |
2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Dimension
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Thickness | 0.5 mm Show Material materials with Thickness of 0.5 mm | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | 0.5 mm | Coil, Sheet, Strip |
3.0 mm Show Material materials with Thickness of 3.0 mm | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | 3.0 mm | Coil, Sheet, Strip |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending angle 180° | 1 °/t Show Material materials with Bending angle 180° of 1 °/t | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
1.5 °/t Show Material materials with Bending angle 180° of 1.5 °/t | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
2.0 °/t Show Material materials with Bending angle 180° of 2.0 °/t | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Bending angle 90° | 0.5 °/t Show Material materials with Bending angle 90° of 0.5 °/t | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
0.5 °/t Show Material materials with Bending angle 90° of 0.5 °/t | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |||
1.0 °/t Show Material materials with Bending angle 90° of 1.0 °/t | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
1.5 °/t Show Material materials with Bending angle 90° of 1.5 °/t | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
2.0 °/t Show Material materials with Bending angle 90° of 2.0 °/t | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Elastic modulus | 68.6 GPa Show Material materials with Elastic modulus of 68.6 GPa | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Hardness, Brinell | 54.0 [-] Show Material materials with Hardness, Brinell of 54.0 [-] | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 54.0 [-] Show Material materials with Hardness, Brinell of 54.0 [-] | H34 | EN 573-3 | Flat | ||
Hardness, HBW | 54 [-] Show Material materials with Hardness, HBW of 54 [-] | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 26.5 GPa Show Material materials with Shear modulus of 26.5 GPa | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Tensile strength | 20.0 °C | 175.0 - 215.0 MPa Show Material materials with Tensile strength of 175.0 - 215.0 MPa | H34 | EN 573-3 | Flat | Transverse |
20.0 °C | 175.0 - 215.0 MPa Show Material materials with Tensile strength of 175.0 - 215.0 MPa | H34 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Strip, Sheet, Plate, Coil, Sheet, Strip, Flat | ||
Yield strength | 135.0 MPa Show Material materials with Yield strength of 135.0 MPa | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | RP02 | |
135 MPa Show Material materials with Yield strength of 135 MPa | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |||
20.0 °C | 135.0 MPa Show Material materials with Yield strength of 135.0 MPa | H34 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 135.0 MPa Show Material materials with Yield strength of 135.0 MPa | H34 | EN 573-3 | Flat | RP02 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
100 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
100 °C | 0.000024 1/K Show Material materials with Coefficient of thermal expansion of 0.000024 1/K | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | 20-100°C | |
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Melting point | 620.0 - 650.0 °C Show Material materials with Melting point of 620.0 - 650.0 °C | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
625.0 - 650.0 °C Show Material materials with Melting point of 625.0 - 650.0 °C | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Specific heat capacity | 879.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | ||||
Thermal conductivity | 170.0 - 190.0 W/(m·K) Show Material materials with Thermal conductivity of 170.0 - 190.0 W/(m·K) | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
192 W/(m·K) Show Material materials with Thermal conductivity of 192 W/(m·K) | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |||
193 W/(m·K) Show Material materials with Thermal conductivity of 193 W/(m·K) | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Electrical
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Electrical conductivity | 23000000.0 - 26000000.0 S/m Show Material materials with Electrical conductivity of 23000000.0 - 26000000.0 S/m | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate |
29000000.0 S/m Show Material materials with Electrical conductivity of 29000000.0 S/m | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
Electrical resistivity | 3.4e-08 Ω·m Show Material materials with Electrical resistivity of 3.4e-08 Ω·m | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
3.45e-08 Ω·m Show Material materials with Electrical resistivity of 3.45e-08 Ω·m | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
3.85e-08 - 4.35e-08 Ω·m Show Material materials with Electrical resistivity of 3.85e-08 - 4.35e-08 Ω·m | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | H34 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.1 % Show Material materials with Chromium of 0.1 % | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Copper | 0.2 % Show Material materials with Copper of 0.2 % | H34 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.2 % Show Material materials with Copper of 0.2 % | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Iron | 0.7 % Show Material materials with Iron of 0.7 % | H34 | EN 573-3 | Flat |
0.70 % Show Material materials with Iron of 0.70 % | H34 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
0.7 % Show Material materials with Iron of 0.7 % | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Magnesium | 1.1 - 1.8 % Show Material materials with Magnesium of 1.1 - 1.8 % | H34 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Coil, Sheet, Strip |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | H34 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.1 % Show Material materials with Manganese of 0.1 % | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
0.3 % Show Material materials with Manganese of 0.3 % | H34 | EN 573-3 | Flat | |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | H34 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.4 % Show Material materials with Silicon of 0.4 % | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H34 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.25 % Show Material materials with Zinc of 0.25 % | H34 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Technological properties
Property | ||
---|---|---|
Anodizing | Very Good (anodizing quality) | |
Application areas | Roofing: Single sheet, Sheets for composites/ sandwich Panels; Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Anodizing quality; Tubes: Industrial tubes, Pipes; Food can: Body, Lids | |
Brazing | Good | |
Corrosion properties | Excellent | |
General machinability | Fair | |
Welding | Excellent | |
Workability | Very Good |