General
Property | Value | Condition | Related Standards |
---|---|---|---|
Density | 2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | H111 | EN 573-3, EN 485 |
Mechanical
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastic modulus | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H111 | EN 573-3, EN 485 | |
Hardness, Brinell | 25.0 [-] Show Material materials with Hardness, Brinell of 25.0 [-] | H111 | EN 573-3, EN 485 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||
Tensile strength | 85.0 MPa Show Material materials with Tensile strength of 85.0 MPa | H111 | EN 573-3, EN 485 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | H111 | EN 573-3, EN 485 | |
100 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | H111 | EN 573-3, EN 485 | ||
Melting point | 640.0 - 655.0 °C Show Material materials with Melting point of 640.0 - 655.0 °C | H111 | EN 573-3, EN 485 | ||
Specific heat capacity | 920.0 J/(kg·K) Show Material materials with Specific heat capacity of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | |||
Thermal conductivity | 210.0 - 220.0 W/(m·K) Show Material materials with Thermal conductivity of 210.0 - 220.0 W/(m·K) | H111 | EN 573-3, EN 485 |
Electrical
Property | Value | Condition | Related Standards |
---|---|---|---|
Electrical conductivity | 34000000.0 - 35000000.0 S/m Show Material materials with Electrical conductivity of 34000000.0 - 35000000.0 S/m | H111 | EN 573-3, EN 485 |
Electrical resistivity | 2.86e-08 - 2.94e-08 Ω·m Show Material materials with Electrical resistivity of 2.86e-08 - 2.94e-08 Ω·m | H111 | EN 573-3, EN 485 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | H111 | EN 573-3, EN 485 |
Copper | 0.1 % Show Material materials with Copper of 0.1 % | H111 | EN 573-3, EN 485 |
Iron | 0.5 - 1.0 % Show Material materials with Iron of 0.5 - 1.0 % | H111 | EN 573-3, EN 485 |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | H111 | EN 573-3, EN 485 |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | H111 | EN 573-3, EN 485 |
Silicon | 0.4 - 0.8 % Show Material materials with Silicon of 0.4 - 0.8 % | H111 | EN 573-3, EN 485 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | H111 | EN 573-3, EN 485 |