General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | H14 | EN 573-3, EN 485, EN 541, EN 683 | ||
20.0 °C | 2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H14 | EN 573-3, EN 485, EN 541, EN 683 | |||
Elongation | 1.0 % Show Material materials with Elongation of 1.0 % | H14 | EN 573-3, EN 683 | A50 | ||
2.0 % Show Material materials with Elongation of 2.0 % | H14 | EN 573-3, EN 485, EN 541 | A50 | |||
3.0 % Show Material materials with Elongation of 3.0 % | H14 | EN 573-3, EN 485 | A50 | |||
4.0 % Show Material materials with Elongation of 4.0 % | H14 | EN 573-3, EN 485 | A50 | |||
5.0 % Show Material materials with Elongation of 5.0 % | H14 | EN 573-3, EN 485 | A50 | |||
20.0 °C | 3.0 % Show Material materials with Elongation of 3.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 4.0 % Show Material materials with Elongation of 4.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 5.0 % Show Material materials with Elongation of 5.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Hardness, Brinell | 41.0 [-] Show Material materials with Hardness, Brinell of 41.0 [-] | H14 | EN 573-3, EN 485 | |||
20.0 °C | 40.0 [-] Show Material materials with Hardness, Brinell of 40.0 [-] | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Tensile strength | 120.0 - 170.0 MPa Show Material materials with Tensile strength of 120.0 - 170.0 MPa | H14 | EN 573-3, EN 683 | |||
125.0 - 165.0 MPa Show Material materials with Tensile strength of 125.0 - 165.0 MPa | H14 | EN 573-3, EN 485, EN 541 | ||||
20.0 °C | 130.0 - 170.0 MPa Show Material materials with Tensile strength of 130.0 - 170.0 MPa | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | H14 | EN 573-3, EN 485, EN 541, EN 683 | ||
100 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | H14 | EN 573-3, EN 485, EN 541, EN 683 | |||
Melting point | 640.0 - 655.0 °C Show Material materials with Melting point of 640.0 - 655.0 °C | H14 | EN 573-3, EN 485, EN 541, EN 683 | |||
Specific heat capacity | 920.0 J/(kg·K) Show Material materials with Specific heat capacity of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Thermal conductivity | 20.0 °C | 210.0 - 220.0 W/(m·K) Show Material materials with Thermal conductivity of 210.0 - 220.0 W/(m·K) | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 34000000.0 - 35000000.0 S/m Show Material materials with Electrical conductivity of 34000000.0 - 35000000.0 S/m | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Electrical resistivity | 2.86e-08 - 2.94e-08 Ω·m Show Material materials with Electrical resistivity of 2.86e-08 - 2.94e-08 Ω·m | H14 | EN 573-3, EN 485, EN 541, EN 683 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | H14 | EN 573-3, EN 485, EN 541, EN 683 | |
Copper | 0.1 % Show Material materials with Copper of 0.1 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Iron | 0.5 - 1.0 % Show Material materials with Iron of 0.5 - 1.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | H14 | EN 573-3, EN 485, EN 541, EN 683 | |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Silicon | 0.4 - 0.8 % Show Material materials with Silicon of 0.4 - 0.8 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Titanium | 0.05 Show Material materials with Titanium of 0.05 | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |