EN 573-3 Grade 3.0515 O

Want to keep this datasheet? Save it now in your required format

Description

The alloy AlMn1 is an Al-Mn alloy, which belongs to the nature-hard aluminum materials. Mn increases the strength compared with pure aluminium, but it does not impair the corrosion resistance. The alloy belongs to the nature-hard aluminum materials. A strength increase can only occur by cold forming. It is very well formable, very well corrosion resistant and weldable. In these characteristics it resembles the pure aluminium, but with the attainable strength it exceeds this. The alloy AlMn1 has a increased heat resistance compared with pure aluminium, as result of the of the Mn-additive (inhibits recrystallisation). Application: In the building industry for roofings, as outer skin of buildings, in the apparatus and tank construction as heat exchanger (bank of tubes, profiles, gilled pipes, sheet metals), for radiators, air conditioning systems, pipings for compressed gas tanks, for tanks according VdTUEV Werkstoffblaetter, as antennas for radio relay link and satellite communication (mirror) for technical flow pressed parts, for solid rivets, for generally metal-describe, in food industry (including commercial devices), in the construction of vehicles (including tank cars) and as packing (sheet metal packings generally).

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.73 g/cm³

Show Material materials with Density of 2.73 g/cm³

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

20.0 °C

2.73 g/cm³

Show Material materials with Density of 2.73 g/cm³

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Sheet, Strip, Tube, Wire

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending Fatigue Strength

50.0 MPa

Show Material materials with Bending Fatigue Strength of 50.0 MPa

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Bending angle 180°

1.0 °/t

Show Material materials with Bending angle 180° of 1.0 °/t

O

EN 573-3, EN 485

Bending angle 90°

1.0 °/t

Show Material materials with Bending angle 90° of 1.0 °/t

O

EN 573-3, EN 485

1.5 °/t

Show Material materials with Bending angle 90° of 1.5 °/t

O

EN 573-3, EN 485

Elastic modulus

69.5 GPa

Show Material materials with Elastic modulus of 69.5 GPa

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastic modulus of 60.0 - 65.0 GPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Sheet, Strip, Tube, Wire

Elongation

-196.0 °C

46.0 %

Show Material materials with Elongation of 46.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

-80.0 °C

42.0 %

Show Material materials with Elongation of 42.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

-20.0 °C

41.0 %

Show Material materials with Elongation of 41.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

7.0 %

Show Material materials with Elongation of 7.0 %

O

EN 573-3, EN 546

A50

8.0 %

Show Material materials with Elongation of 8.0 %

O

EN 573-3, EN 546

A50

12.0 %

Show Material materials with Elongation of 12.0 %

O

EN 573-3, EN 546, EN 683

A50

15.0 %

Show Material materials with Elongation of 15.0 %

O

EN 573-3, EN 546, EN 683

A50

17.0 %

Show Material materials with Elongation of 17.0 %

O

EN 573-3, EN 485

A50

18.0 %

Show Material materials with Elongation of 18.0 %

O

EN 573-3, EN 683

A50

19.0 %

Show Material materials with Elongation of 19.0 %

O

EN 573-3, EN 485

A50

20.0 %

Show Material materials with Elongation of 20.0 %

O

EN 573-3, EN 754, EN 755

A50

21.0 %

Show Material materials with Elongation of 21.0 %

O

EN 573-3, EN 485

A50

24.0 %

Show Material materials with Elongation of 24.0 %

O

EN 573-3, EN 485

A50

25.0 %

Show Material materials with Elongation of 25.0 %

O

EN 573-3, EN 485, EN 754, EN 755

A100

28.0 %

Show Material materials with Elongation of 28.0 %

O

EN 573-3, EN 485

A50

35.0 %

Show Material materials with Elongation of 35.0 %

O

EN 573-3, EN 1301

20.0 °C

16.0 %

Show Material materials with Elongation of 16.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Wire

A100

20.0 °C

19.0 %

Show Material materials with Elongation of 19.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod

A10

20.0 °C

20.0 %

Show Material materials with Elongation of 20.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Tube, Wire

A10

20.0 °C

21.0 %

Show Material materials with Elongation of 21.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Sheet, Strip

A10

20.0 °C

22.0 %

Show Material materials with Elongation of 22.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Tube

20.0 °C

24.0 %

Show Material materials with Elongation of 24.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Sheet, Strip

20.0 °C

40.0 %

Show Material materials with Elongation of 40.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

100.0 °C

43.0 %

Show Material materials with Elongation of 43.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

150.0 °C

47.0 %

Show Material materials with Elongation of 47.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

200.0 °C

60.0 %

Show Material materials with Elongation of 60.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

260.0 °C

65.0 %

Show Material materials with Elongation of 65.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

320.0 °C

70.0 %

Show Material materials with Elongation of 70.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

370.0 °C

70.0 %

Show Material materials with Elongation of 70.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Hardness, Brinell

27.0 [-]

Show Material materials with Hardness, Brinell of 27.0 [-]

O

EN 573-3, EN 485

20.0 °C

25.0 [-]

Show Material materials with Hardness, Brinell of 25.0 [-]

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Wire

20.0 °C

28.0 [-]

Show Material materials with Hardness, Brinell of 28.0 [-]

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Sheet, Strip

20.0 °C

30.0 [-]

Show Material materials with Hardness, Brinell of 30.0 [-]

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

26.1 GPa

Show Material materials with Shear modulus of 26.1 GPa

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

20.0 °C

24.0 - 26.5 GPa

Show Material materials with Shear modulus of 24.0 - 26.5 GPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Sheet, Strip, Tube, Wire

Tensile strength

-196.0 °C

232.0 MPa

Show Material materials with Tensile strength of 232.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

-80.0 °C

137.0 MPa

Show Material materials with Tensile strength of 137.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

-20.0 °C

119.0 MPa

Show Material materials with Tensile strength of 119.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

80.0 - 130.0 MPa

Show Material materials with Tensile strength of 80.0 - 130.0 MPa

O

EN 573-3, EN 546, EN 683

90.0 - 130.0 MPa

Show Material materials with Tensile strength of 90.0 - 130.0 MPa

O

EN 573-3, EN 485

95.0 - 130.0 MPa

Show Material materials with Tensile strength of 95.0 - 130.0 MPa

O

EN 573-3, EN 754

95.0 - 135.0 MPa

Show Material materials with Tensile strength of 95.0 - 135.0 MPa

O

EN 573-3, EN 755

130.0 MPa

Show Material materials with Tensile strength of 130.0 MPa

O

EN 573-3, EN 1301

20.0 °C

90.0 - 140.0 MPa

Show Material materials with Tensile strength of 90.0 - 140.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Sheet, Strip

20.0 °C

95.0 MPa

Show Material materials with Tensile strength of 95.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Tube, Wire

20.0 °C

112.0 MPa

Show Material materials with Tensile strength of 112.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

100.0 °C

91.0 MPa

Show Material materials with Tensile strength of 91.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

150.0 °C

77.0 MPa

Show Material materials with Tensile strength of 77.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

200.0 °C

57.0 MPa

Show Material materials with Tensile strength of 57.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

260.0 °C

47.0 MPa

Show Material materials with Tensile strength of 47.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

320.0 °C

28.0 MPa

Show Material materials with Tensile strength of 28.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

370.0 °C

19.0 MPa

Show Material materials with Tensile strength of 19.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

20 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

100 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Melting point

645.0 - 655.0 °C

Show Material materials with Melting point of 645.0 - 655.0 °C

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Specific heat capacity

893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 J/(kg·K)

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

20.0 °C

893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 J/(kg·K)

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Sheet, Strip, Tube, Wire

Thermal conductivity

20.0 °C

160.0 - 200.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 - 200.0 W/(m·K)

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

22000000.0 - 28000000.0 S/m

Show Material materials with Electrical conductivity of 22000000.0 - 28000000.0 S/m

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Electrical resistivity

3.57e-08 - 4.55e-08 Ω·m

Show Material materials with Electrical resistivity of 3.57e-08 - 4.55e-08 Ω·m

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Copper

0.1 %

Show Material materials with Copper of 0.1 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Iron

0.7 %

Show Material materials with Iron of 0.7 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Sheet, Strip, Tube, Wire

0.70 %

Show Material materials with Iron of 0.70 %

O

EN 573-3, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Magnesium

0.3 %

Show Material materials with Magnesium of 0.3 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Manganese

0.9 - 1.5 %

Show Material materials with Manganese of 0.9 - 1.5 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Titanium

0.1

Show Material materials with Titanium of 0.1

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Rod, Sheet, Strip, Tube, Wire

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

O

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 1301, EN 485, EN 546, EN 683, EN 754, EN 755

Rod, Sheet, Strip, Tube, Wire

Technological properties

Property
Workability

Good workability.