General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ | H18 | EN 573-3, EN 485, EN 754 | ||
20.0 °C | 2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending angle 90° | 1.5 °/t Show Material materials with Bending angle 90° of 1.5 °/t | H18 | EN 573-3, EN 485 | |||
2.5 °/t Show Material materials with Bending angle 90° of 2.5 °/t | H18 | EN 573-3, EN 485 | ||||
3.0 °/t Show Material materials with Bending angle 90° of 3.0 °/t | H18 | EN 573-3, EN 485 | ||||
Elastic modulus | 69.5 GPa Show Material materials with Elastic modulus of 69.5 GPa | H18 | EN 573-3, EN 485, EN 754 | |||
20.0 °C | 60.0 - 65.0 GPa Show Material materials with Elastic modulus of 60.0 - 65.0 GPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire | ||
Elongation | 1.0 % Show Material materials with Elongation of 1.0 % | H18 | EN 573-3, EN 485 | A50 | ||
2.0 % Show Material materials with Elongation of 2.0 % | H18 | EN 573-3, EN 485, EN 754 | A50 | |||
4.0 % Show Material materials with Elongation of 4.0 % | H18 | EN 573-3, EN 754 | A100 | |||
20.0 °C | 1.0 % Show Material materials with Elongation of 1.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire | A100 | |
20.0 °C | 2.0 % Show Material materials with Elongation of 2.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 3.0 % Show Material materials with Elongation of 3.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube, Wire | A10 | |
20.0 °C | 3.0 % Show Material materials with Elongation of 3.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
20.0 °C | 4.0 % Show Material materials with Elongation of 4.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | ||
Hardness, Brinell | 58.0 [-] Show Material materials with Hardness, Brinell of 58.0 [-] | H18 | EN 573-3, EN 485 | |||
20.0 °C | 50.0 [-] Show Material materials with Hardness, Brinell of 50.0 [-] | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | ||
20.0 °C | 55.0 [-] Show Material materials with Hardness, Brinell of 55.0 [-] | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | ||
20.0 °C | 57.0 [-] Show Material materials with Hardness, Brinell of 57.0 [-] | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 26.1 GPa Show Material materials with Shear modulus of 26.1 GPa | H18 | EN 573-3, EN 485, EN 754 | |||
20.0 °C | 25.0 GPa Show Material materials with Shear modulus of 25.0 GPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire | ||
Tensile strength | 185.0 MPa Show Material materials with Tensile strength of 185.0 MPa | H18 | EN 573-3, EN 485, EN 754 | |||
20.0 °C | 185.0 MPa Show Material materials with Tensile strength of 185.0 MPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube, Wire | ||
20.0 °C | 190.0 - 230.0 MPa Show Material materials with Tensile strength of 190.0 - 230.0 MPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | -50 °C | 2.18e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.18e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | |
-50.0 °C | 2.18e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.18e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
20 °C | 2.18e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.18e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
20 °C | 2.36e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
20 °C | 2.45e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.45e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
20 °C | 2.55e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.55e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
100 °C | 2.36e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
100.0 °C | 2.36e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
200 °C | 2.45e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.45e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
200.0 °C | 2.45e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.45e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
300 °C | 2.55e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.55e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
300.0 °C | 2.55e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.55e-05 1/K | H18 | EN 573-3, EN 485, EN 754, DIN 1725-1, EN 573-4 | Rod, Flat, Tube, Wire | ||
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Melting point | 630.0 - 650.0 °C Show Material materials with Melting point of 630.0 - 650.0 °C | H18 | EN 573-3, EN 485, EN 754 | |||
Specific heat capacity | 20.0 °C | 879.0 J/(kg·K) Show Material materials with Specific heat capacity of 879.0 J/(kg·K) | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire | |
Thermal conductivity | 20.0 °C | 160.0 - 220.0 W/(m·K) Show Material materials with Thermal conductivity of 160.0 - 220.0 W/(m·K) | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754 | Rod, Flat, Tube, Wire |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 23000000.0 - 31000000.0 S/m Show Material materials with Electrical conductivity of 23000000.0 - 31000000.0 S/m | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754 | Rod, Flat, Tube, Wire |
Electrical resistivity | 3.23e-08 - 4.35e-08 Ω·m Show Material materials with Electrical resistivity of 3.23e-08 - 4.35e-08 Ω·m | H18 | EN 573-3, EN 485, EN 754 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754 | Rod, Flat, Tube, Wire |
Copper | 0.05 % Show Material materials with Copper of 0.05 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire |
0.2 % Show Material materials with Copper of 0.2 % | H18 | EN 573-3, EN 485, EN 754 | ||
Iron | 0.45 % Show Material materials with Iron of 0.45 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire |
0.70 % Show Material materials with Iron of 0.70 % | H18 | EN 573-3, EN 485, EN 754 | ||
Magnesium | 0.7 - 1.1 % Show Material materials with Magnesium of 0.7 - 1.1 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire |
1.1 - 1.8 % Show Material materials with Magnesium of 1.1 - 1.8 % | H18 | EN 573-3, EN 485, EN 754 | ||
Manganese | 0.15 % Show Material materials with Manganese of 0.15 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire |
0.3 % Show Material materials with Manganese of 0.3 % | H18 | EN 573-3, EN 485, EN 754 | ||
Silicon | 0.3 % Show Material materials with Silicon of 0.3 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire |
0.4 % Show Material materials with Silicon of 0.4 % | H18 | EN 573-3, EN 485, EN 754 | ||
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Flat, Tube, Wire |
0.25 % Show Material materials with Zinc of 0.25 % | H18 | EN 573-3, EN 485, EN 754 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |