General
Property | Value | Condition | Related Standards |
---|---|---|---|
Density | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | F | EN 573-3, EN 1715-3, EN 570 |
Mechanical
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastic modulus | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | F | EN 573-3, EN 1715-3, EN 570 | |
Hardness, Brinell | 18.0 [-] Show Material materials with Hardness, Brinell of 18.0 [-] | F | EN 573-3, EN 570 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||
Shear modulus | 25.9 GPa Show Material materials with Shear modulus of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | ||
Tensile strength | 75.0 - 85.0 MPa Show Material materials with Tensile strength of 75.0 - 85.0 MPa | F | EN 573-3, EN 1715-3 |
Thermal
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Coefficient of thermal expansion | -50 °C | 2.18e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.18e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 |
20 °C | 2.18e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.18e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | |
20 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | |
20 °C | 2.45e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.45e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | |
20 °C | 2.55e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.55e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | |
100 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | |
200 °C | 2.45e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.45e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | |
300 °C | 2.55e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.55e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | |
Melting point | 660.0 °C Show Material materials with Melting point of 660.0 °C | F | EN 573-3, EN 1715-3, EN 570 | |
Specific heat capacity | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | F | EN 573-3, EN 1715-3, EN 570 | |
Thermal conductivity | 232 W/(m·K) Show Material materials with Thermal conductivity of 232 W/(m·K) | F | EN 573-3, EN 1715-3, EN 570 |
Electrical
Property | Value | Condition | Related Standards |
---|---|---|---|
Electrical conductivity | 37500000.0 - 37700000.0 S/m Show Material materials with Electrical conductivity of 37500000.0 - 37700000.0 S/m | F | EN 573-3, EN 1715-3, EN 570 |
Electrical resistivity | 2.65e-08 - 2.67e-08 Ω·m Show Material materials with Electrical resistivity of 2.65e-08 - 2.67e-08 Ω·m | F | EN 573-3, EN 1715-3, EN 570 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 99.98 % Show Material materials with Aluminium of 99.98 % | F | EN 573-3, EN 1715-3, EN 570 |
Copper | 0.003 % Show Material materials with Copper of 0.003 % | F | EN 573-3, EN 1715-3, EN 570 |
Iron | 0.006 % Show Material materials with Iron of 0.006 % | F | EN 573-3, EN 1715-3, EN 570 |
Silicon | 0.01 % Show Material materials with Silicon of 0.01 % | F | EN 573-3, EN 1715-3, EN 570 |
Titanium | 0.003 % Show Material materials with Titanium of 0.003 % | F | EN 573-3, EN 1715-3, EN 570 |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % | F | EN 573-3, EN 1715-3, EN 570 |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |