General
Property | Temperature | Value | |
---|---|---|---|
Density | 23.0 °C | 14.8 g/cm³ Show Supplier Material materials with Density of 14.8 g/cm³ | |
Binder | Cobalt binder | ||
Grain structure | Fine grain size |
Mechanical
Property | Temperature | Value |
---|---|---|
Compressive strength | 23.0 °C | 5000 MPa Show Supplier Material materials with Compressive strength of 5000 MPa |
Elastic modulus | 23.0 °C | 590 GPa Show Supplier Material materials with Elastic modulus of 590 GPa |
Hardness, Rockwell A | 23.0 °C | 90.9 [-] Show Supplier Material materials with Hardness, Rockwell A of 90.9 [-] |
Hardness, Vickers, 10 | 23.0 °C | 1480 [-] Show Supplier Material materials with Hardness, Vickers, 10 of 1480 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 11.4 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 11.4 MPa·√m |
Tensile strength, transverse | 23.0 °C | 2900 MPa Show Supplier Material materials with Tensile strength, transverse of 2900 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.1E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.1E-6 1/K |
Thermal conductivity | 23.0 °C | 85 W/(m·K) Show Supplier Material materials with Thermal conductivity of 85 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Cobalt | 8 % Show Supplier Material materials with Cobalt of 8 % | as binder | |
Tungsten | WC balance |
Technological properties
Property | ||
---|---|---|
Certifications | Compliant with FDA food contact notification number 586 - 591. |