General
Property | Temperature | Value | |
---|---|---|---|
Density | 23.0 °C | 12.45 g/cm³ Show Supplier Material materials with Density of 12.45 g/cm³ | |
Binder | Cobalt binder | ||
Grain structure | Medium grain size |
Mechanical
Property | Temperature | Value |
---|---|---|
Compressive strength | 23.0 °C | 6000 MPa Show Supplier Material materials with Compressive strength of 6000 MPa |
Elastic modulus | 23.0 °C | 530 GPa Show Supplier Material materials with Elastic modulus of 530 GPa |
Hardness, Rockwell A | 23.0 °C | 91.5 [-] Show Supplier Material materials with Hardness, Rockwell A of 91.5 [-] |
Hardness, Vickers | 23.0 °C | 1560 [-] Show Supplier Material materials with Hardness, Vickers of 1560 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 10.7 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 10.7 MPa·√m |
Tensile strength, transverse | 23.0 °C | 2150 MPa Show Supplier Material materials with Tensile strength, transverse of 2150 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.9E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.9E-6 1/K |
Thermal conductivity | 23.0 °C | 55 W/(m·K) Show Supplier Material materials with Thermal conductivity of 55 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Cobalt | 9 % Show Supplier Material materials with Cobalt of 9 % | as binder | |
Tungsten | WC balance |
Technological properties
Property |
---|