Description

CTS24Z, the special high-performance grade for the roughing of titanium and heat-resistant alloys. Even higher fracture toughness than CTS18D and CTS20D, with approximately the same hardness.

Related Standards

This material data has been provided by Ceratizit.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

14.1 g/cm³

Show Supplier Material materials with Density of 14.1 g/cm³

Grain structure

Submicron (0,5µm - 0,8µm)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

549 GPa

Show Supplier Material materials with Elastic modulus of 549 GPa

Hardness, Rockwell A

23.0 °C

91.7 [-]

Show Supplier Material materials with Hardness, Rockwell A of 91.7 [-]

Hardness, Vickers, 10

23.0 °C

1590 [-]

Show Supplier Material materials with Hardness, Vickers, 10 of 1590 [-]

EN ISO 6507-1

Hardness, Vickers, 30

23.0 °C

1570 [-]

Show Supplier Material materials with Hardness, Vickers, 30 of 1570 [-]

EN ISO 6507-1

Plane-Strain Fracture Toughnes

23.0 °C

11.3 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 11.3 MPa·√m

ISO 28079

Poisson's ratio

23.0 °C

0.22 [-]

Show Supplier Material materials with Poisson's ratio of 0.22 [-]

Tensile strength, transverse

23.0 °C

4000 MPa

Show Supplier Material materials with Tensile strength, transverse of 4000 MPa

DIN EN ISO 7438

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

5.4E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.4E-6 1/K

Specific heat capacity

23.0 °C

0.21 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 0.21 J/(kg·K)

Thermal conductivity

23.0 °C

62 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 62 W/(m·K)

Thermal diffusivity

23.0 °C

21 mm²/s

Show Supplier Material materials with Thermal diffusivity of 21 mm²/s

Chemical properties

PropertyValueComment

Cobalt

12 %

Show Supplier Material materials with Cobalt of 12 %

as binder

Other

1.49 %

Show Supplier Material materials with Other of 1.49 %

Tungsten

WC balance