TSF22

Want to keep this datasheet? Save it now in your required format

Description

TSF22: ultrafine carbide grade for HSC machining of tempered steels with a hardness of > 60 HRC and abrasive aluminium alloys.

Related Standards

This material data has been provided by Ceratizit.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

14.55 g/cm³

Show Supplier Material materials with Density of 14.55 g/cm³

Grain structure

Ultrafine (0,2µm - 0,5µm)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

596 GPa

Show Supplier Material materials with Elastic modulus of 596 GPa

Hardness, Rockwell A

23.0 °C

93.7 [-]

Show Supplier Material materials with Hardness, Rockwell A of 93.7 [-]

Hardness, Vickers, 10

23.0 °C

1970 [-]

Show Supplier Material materials with Hardness, Vickers, 10 of 1970 [-]

EN ISO 6507-1

Hardness, Vickers, 30

23.0 °C

1930 [-]

Show Supplier Material materials with Hardness, Vickers, 30 of 1930 [-]

EN ISO 6507-1

Plane-Strain Fracture Toughnes

23.0 °C

9.2 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 9.2 MPa·√m

ISO 28079

Poisson's ratio

23.0 °C

0.21 [-]

Show Supplier Material materials with Poisson's ratio of 0.21 [-]

Tensile strength, transverse

23.0 °C

4400 MPa

Show Supplier Material materials with Tensile strength, transverse of 4400 MPa

DIN EN ISO 7438

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

5.02E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.02E-6 1/K

Chemical properties

PropertyValueComment

Cobalt

8.2 %

Show Supplier Material materials with Cobalt of 8.2 %

as binder

Other

0.82 %

Show Supplier Material materials with Other of 0.82 %

Tungsten

WC balance