General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 56.0 % Show Supplier Material materials with Bio-based content of 56.0 % | dry | ASTM D6866-12 Method B |
Density | 1.05 g/cm³ Show Supplier Material materials with Density of 1.05 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 1 GPa Show Supplier Material materials with Elastic modulus of 1 GPa | conditioned | ISO 527-1/-2 | |
2 GPa Show Supplier Material materials with Elastic modulus of 2 GPa | dry | ISO 527-1/-2 | ||
Elongation | 30 % Show Supplier Material materials with Elongation of 30 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongation of 50 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | 6 % Show Supplier Material materials with Elongation at yield of 6 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | conditioned | ISO 527-1/-2 | ||
Impact strength, Charpy notched | -30 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | dry | ISO 179/1eA |
23 °C | 75 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 75 kJ/m² | dry, conditioned | ISO 179/1eA | |
Tensile strength | 35 MPa Show Supplier Material materials with Tensile strength of 35 MPa | conditioned | ISO 527-1/-2 | |
50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dielectric strength | 36 kV/mm Show Supplier Material materials with Dielectric strength of 36 kV/mm | dry | IEC 60243-1 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt mass-flow rate | 290 °C | 28.0 g/10min Show Supplier Material materials with Melt mass-flow rate of 28.0 g/10min | dry | ISO 1133 | |
Melt volume-flow rate | 290 °C | 32 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 32 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.8 % Show Supplier Material materials with Shrinkage of 1.8 % | dry | ISO 294-4 | Normal | |
2.8 % Show Supplier Material materials with Shrinkage of 2.8 % | dry | ISO 294-4 | Parallel |