General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.4 g/cm³ Show Supplier Material materials with Density of 1.4 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 15.8 GPa Show Supplier Material materials with Elastic modulus of 15.8 GPa | dry | ISO 527-1/-2 | |
Elongation | 3.3 % Show Supplier Material materials with Elongation of 3.3 % | dry | ISO 527-1/-2 | |
Flexural modulus | 13.6 GPa Show Supplier Material materials with Flexural modulus of 13.6 GPa | dry | ISO 178 | |
Impact strength, Charpy unnotched | 23 °C | 20.1 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 20.1 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 167 MPa Show Supplier Material materials with Tensile strength of 167 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Thickness | Testing Standard |
---|---|---|---|---|
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | 0.75 mm | UL746B |
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.75 mm | UL746B |
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | 0.75 mm | UL746B |
Thermal diffusivity | 8.99e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 8.99e-08 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 4800 Ω/sq Show Supplier Material materials with Surface resistivity of 4800 Ω/sq | conditioned | IEC 62631-3-2 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density of melt | 1110 g/cm³ Show Supplier Material materials with Density of melt of 1110 g/cm³ | dry | - |
Specific heat capacity melt | 2830.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2830.0 J/(kg·K) | dry | - |
Thermal conductivity of melt | 0.28 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.28 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber and Carbon Fiber |